Microstructure and Mechanical Properties of Dissimilar Friction Stir Welded T-Lap Joints Between AA5083 and AA7020
Janusz Torzewski1, Tomasz Helt1, Robert Kosturek1
1Faculty of Mechanical Engineering, Military University of Technology, gen. S. Kaliskiego 2 Str., 00-908 Warsaw, Poland.
Abstract:
This paper investigates the microstructural evolution and mechanical performance of dissimilar friction stir-welded (FSW) T-joints produced from AA5083-H111 and AA7020-T651 aluminium alloys. The study focuses on the effects of tool rotational speed, traverse speed, and tool pin length on joint quality and mechanical strength. Welding experiments were conducted at two rotational speeds (400 and 700 rpm) and three traverse speeds (50, 100, and 200 mm/min) using two Triflute tools with pin lengths of 4.8 mm and 6.8 mm. The welded joints were examined by macro- and microstructural observations, microhardness measurements, and bending tests performed under pull-out loading conditions. The results showed that the use of the longer pin significantly improved material mixing and reduced the extent of internal defects, resulting in higher bending strength. Increasing the traverse speed improved the mechanical performance, whereas an excessively high rotational speed reduced joint strength due to increased heat input and unfavourable microstructural changes. Microhardness profiles showed no reduction in hardness within the heat-affected zones relative to the base materials and indicated localised hardening in the stir zone. For the investigated material configuration and tool geometries, the highest joint strength was obtained at a rotational speed of 400 rpm and a traverse speed of 200 mm/min using the longer-pin tool. The study confirms the critical role of process parameter optimisation and tool geometry in producing high-quality dissimilar FSW T-joints suitable for lightweight structural applications.
More Related Videos
Related Concept Videos
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used to...
Yield Criteria for Ductile Materials under Plane Stress
The Maximum Shearing Stress Criterion, also known as the...
Bending of Members Made of Several Materials
Hooke's Law determines stress in each material, stating that stress is proportional to strain but varies due to each material's...
Steel Fastening Techniques
Rivets are cylindrical steel fasteners with a specially designed head. During application, rivets are heated until white-hot and then inserted through pre-drilled holes in the steel sections. A pneumatic hammer is used to shape the exposed end into a second head, securing the sections together.
Bolting is another...