Integration of Nickel Adsorption Procedures into the Hydrometallurgical Processing of Laterite Ore: Comparative
Roza Shayakhmetova1, Anar Mukhametzhanova1,2, Almira Kuandykova1,3
1Laboratory of Rare Metals, RSE "National Center of Complex Processing of Mineral Raw Materials of the Republic of Kazakhstan", Zhandossov St., 67, Almaty 050036, Kazakhstan.
Abstract:
Selective Ni(II) recovery from polymetallic sulfate leachates is challenging because of competition from accompanying metal ions, particularly Mg(II). This study systematically evaluated selective Ni(II) recovery using commercial chelating ion-exchange resins and assessed their adsorption performance and regeneration behavior in the context of their integration into a conceptual flowsheet for oxidized nickel ore processing. The ore was characterized by XRF, XRD, and SEM-EDS, while Seplite LSC 495 (bispicolylamine) and Seplite LSC 773 (iminodiacetate) were evaluated using selectivity tests, kinetic and equilibrium studies, FTIR spectroscopy, and adsorption-desorption experiments. Both resins exhibited high selectivity for Ni(II) over Co(II) and Mg(II). Under the optimized conditions, Seplite LSC 773 achieved 99.36 ± 0.08% Ni(II) recovery from the model solution and 98.59 ± 0.36% from the actual leach solution, whereas Seplite LSC 495 achieved 94.62 ± 0.21% and 94.23 ± 0.21%, respectively. The equilibrium data exhibited a Giles S-type profile without reaching a distinct saturation plateau within the investigated concentration range, and the Freundlich model provided the most appropriate description of the data, consistent with adsorption on energetically heterogeneous binding sites. FTIR spectral changes indicated the involvement of the chelating functional groups in Ni(II) binding. Among the regeneration conditions investigated, 20 wt.% H2SO4 provided the highest Ni(II) desorption efficiency; however, desorption remained limited to approximately 42%, indicating that regeneration remains a major constraint on practical application. The experimental findings were incorporated into a conceptual flowsheet integrating sulfuric acid leaching, selective Ni recovery, subsequent Co separation, and MgSO4·7H2O production. Further work should focus on optimizing regeneration, extending cyclic testing, evaluating continuous-flow operation, and validating the integrated process at the pilot scale.
Related Concept Videos
Extraction: Advanced Methods
Ion-Exchange Chromatography
Precipitation Gravimetry
In determining nickel by gravimetric analysis, a precipitant of ethanolic dimethylglyoxime is added to a hot nickel salt solution. This is quickly followed by the dropwise addition of dilute ammonia solution until precipitation occurs. A...
Ion Exchange
Electrodeposition
Electrodeposition can...
Masking and Demasking Agents
There are many masking agents, such as cyanide, fluoride, triethanolamine, thiourea, and 2,3-bis(sulfanyl)propan-1-ol (formerly 2,3-dimercapto-1-propanol), with the masking agent chosen based on the metal...