Intraoral galvanic corrosion: literature review and case report
The Journal of Prosthetic Dentistry
|February 1, 1993
Abstract:
This article reviewed the dental history of a patient with symptomatic electro-chemical reactions after the occlusal relationship of an existing complete gold crown and silver amalgam restoration was changed. A literature review of oral galvanism is presented with diagnostic techniques and treatment options.
Related Concept Videos
Articles linked to this work by shared authors, journal, and citation graph.
Classification of morphologic effects of percutaneous transluminal coronary angioplasty assessed by intravascular ultrasound.
The American journal of cardiology·1992
Relative sensitivity of four noninvasive methods in assessing systolic cardiovascular effects of isoproterenol in healthy volunteers.
Clinical pharmacology and therapeutics·1992
Comparative binding of etretinate and acitretin to plasma proteins and erythrocytes.
Biochemical pharmacology·1992
[Noninvasive quantification and classification of the severity of aortic stenosis using Doppler echocardiography].
Zeitschrift fur Kardiologie·1992
The effect of intermediate altitude on the Army Physical Fitness Test.
Military medicine·1992
Human gingival epithelial cell adhesion and proliferation on Ti-6Al-4V surface biofunctionalized with a nanoceramic thin film: An in vitro study.
The Journal of prosthetic dentistry·2026
Comparative evaluation of large language models in interpreting the scientific literature on intraoral scanners across varying input levels.
The Journal of prosthetic dentistry·2026
Annual review of selected scientific literature: A report of the Committee on Scientific Investigation of the American Academy of Restorative Dentistry.
The Journal of prosthetic dentistry·2026
Clinical performance and prosthetic outcomes in reinforced implant-supported overdentures: A systematic review.
The Journal of prosthetic dentistry·2026
Effect of cement line on radiographic detection accuracy of abutment-prosthesis misfit.
The Journal of prosthetic dentistry·2026
Phosphomimetic statherin-derived peptide protects against intrinsic enamel erosion independently of sodium trimetaphosphate.
European journal of oral sciences·2026
Influence of Illumination Conditions and Cross-Polarization on DSLR-Based Clinical Tooth Color Assessment: A Comparison With Spectrophotometric Measurements.
Journal of esthetic and restorative dentistry : official publication of the American Academy of Esthetic Dentistry ... [et al.]·2026
Early orthopedic treatment of skeletal Class III malocclusion: Correlating dentoskeletal changes with psychosocial outcomes using the modified SEC III protocol and PIDAQ.
Journal of the World federation of orthodontists·2026
Detection of the presence of second mesiobuccal canal in the maxillary first molar with bitewing radiography using MediXpar.
Morphologie : bulletin de l'Association des anatomistes·2026
PLXDC2-OT-peptide Promotes the Odontogenic/Osteogenic Differentiation of SCAPs via the PI3K-AKT Signalling Pathway.
International dental journal·2026