Abstract:
The use of organic active materials in redox flow batteries (RFBs) presents a promising approach to sustainable large-scale energy storage. However, the stability of nonaqueous organic RFB electrolytes is generally limited by degradation reactions that cause capacity fade. These reactions are commonly thought to convert redox-active organics to products that are no longer electrochemically active. Here we uncover an additional pathway leading to capacity fade that involves the supporting electrolyte salt. Capacity fade in nonaqueous RFBs is studied in detail for the 1,2,4-benzotriazin-4-yl radical (1) as a model compound and extended to several other classes of representative redox-active organics. By using symmetrical batteries (1 0/- ∥1 0/+ ), we delineate that capacity fade occurs in a nonlinear (autocatalytic) fashion via acid-induced decomposition of the supporting salt anion PF6 - in the posolyte solution. This is shown to be a universal degradation reaction in the posolyte of nonaqueous RFBs. Although the acidic degradation products are not detrimental to the posolyte, the crossover of acid to the opposite compartment leads to capacity-limiting protonation of the negolyte active material. Replacement of PF6 - with other anions substantially improves the stability of these nonaqueous electrolytes, as demonstrated with a symmetrical RFB based on 0.38 M active material 1 that can be cycled for >69 days with very high capacity retention (fade rate of ≤0.1% per day). The improved understanding of factors determining the lifetime of nonaqueous electrolytes unlocks rational strategies to develop more durable electrochemical energy storage systems.
Videos de Conceptos Relacionados
Batteries and Fuel Cells
Voltaic/Galvanic Cells
Spontaneous redox reactions occur abundantly in nature. The chemical reaction occurring in a disposable AA battery powering our remote controls is one such example of a spontaneous redox reaction. Another example is the immersion of coiled copper wire into an aqueous silver nitrate solution. The reaction shows a gradual, visually impressive color change from colorless to bright blue and the formation of a grey precipitate on the copper wire. In this experiment,...
Voltammetry: Factors Affecting Measurements