非水レドックスフロー電池における容量低下を引き起こす「無害な」ヘキサフルオロリン酸塩

Wenlong Tang1, Jelte S Steen1, Jurjen W Hettinga1

  • 1Stratingh Institute for Chemistry, University of Groningen, Nijenborgh 3, 9747 AG Groningen, The Netherlands.

ACS applied energy materials
|December 26, 2025
PubMed

関連する概念動画

Batteries and Fuel Cells03:12

Batteries and Fuel Cells

A battery is a galvanic cell that is used as a source of electrical power for specific applications. Modern batteries exist in a multitude of forms to accommodate various applications, from tiny button batteries such as those that power wristwatches to the very large batteries used to supply backup energy to municipal power grids. Some batteries are designed for single-use applications and cannot be recharged (primary cells), while others are based on conveniently reversible cell reactions that...
30.6K
Voltaic/Galvanic Cells02:47

Voltaic/Galvanic Cells

Spontaneous Chemical Reactions
Spontaneous redox reactions occur abundantly in nature. The chemical reaction occurring in a disposable AA battery powering our remote controls is one such example of a spontaneous redox reaction. Another example is the immersion of coiled copper wire into an aqueous silver nitrate solution. The reaction shows a gradual, visually impressive color change from colorless to bright blue and the formation of a grey precipitate on the copper wire. In this experiment,...
62.8K
Voltammetry: Factors Affecting Measurements01:21

Voltammetry: Factors Affecting Measurements

A current produced due to the redox reactions of the analyte at the working and auxiliary electrodes is called a faradaic current. The reaction can be divided into two types. The current generated due to the reduction of the analyte is called cathodic current, and it carries a positive charge. In contrast, the current produced by analyte oxidation is known as an anodic current, and it has a negative charge. The applied potential at the working electrode determines the faradaic current flow, and...
500