Abstract:
The controlled formation of high-pressure silicon polymorphs beneath an oxide layer offers a new paradigm for subsurface phase engineering. We systematically compared sharp Berkovich and spherical nanoindentation on 285 nm SiO2-capped Si(100) using Raman spectroscopy and cross-sectional electron microscopy to reveal how contact geometry and oxide constraint govern phase transformation. Sharp indentation initiates R8 (rhombohedral)/BC8 (body-centered-cubic) phase formation at low loads (42 mN), but the high stress concentration promotes early oxide fracture and radial cracking, limiting the continuous crystalline volume. In contrast, spherical indentation delays observable transformation until ∼92 mN, distributing stress more uniformly. Crucially, we identify a "critical loading window" for optimization. While moderate spherical loads (∼200 mN) facilitate highly ordered crystalline recovery with intact interfaces, excessive loads (∼500 mN) exceed the oxide's confinement capacity, favoring collapse into a disordered amorphous state and localized fracture due to the significant volumetric expansion of the intermediate β-Sn phase. Our results confirm that the oxide modulates stress-relaxation kinetics without altering the fundamental 11-12 GPa transformation threshold. These findings explicitly define the operational limits for dielectric confinement, providing a versatile pathway for engineering subsurface crystalline phases with enhanced carrier mobility and sub-bandgap optical absorption for next-generation silicon photonic and sensing platforms.
関連する概念動画
Phase I Oxidative Reactions: Overview
Phase I Reactions: Oxidation of Carbon-Heteroatom and Miscellaneous Systems
In carbon-nitrogen systems, aliphatic and aromatic amines can undergo oxidative reactions. Secondary and tertiary amines, like those found in tricyclic antidepressants, can undergo N-dealkylation, a process that involves the oxidation of the alkyl group. In addition, oxidative...
Phase I Reactions: Oxidation of Aliphatic and Aromatic Carbon-Containing Systems
Oxidation reactions are fundamental in aromatic carbon-containing systems. An example is the hydroxylation of phenobarbital, a process that transforms it into...
Oxidation Numbers
Pyruvate Oxidation
First, the enzyme pyruvate dehydrogenase removes the carboxyl group from pyruvate and releases it as carbon dioxide. The stripped molecule is then oxidized and releases electrons, which are then picked up by NAD+...
What is Genetic Engineering?