超耐用的超长碳纳米管
Yunxiang Bai1,2, Hongjie Yue1, Jin Wang2,3
1Beijing Key Laboratory of Green Chemical Reaction Engineering and Technology, Department of Chemical Engineering, Tsinghua University, Beijing 100084, China.
概括
碳纳米管 (CNT) 具有出色的耐疲劳性,对于材料的寿命至关重要. 它们的断裂时间取决于温度和初始缺陷的形成,
科学领域:
- 材料科学
- 纳米技术
- 机械工程
背景情况:
- 对于确定结构材料的使用寿命而言,耐疲劳性至关重要.
- 碳纳米管 (CNT) 非常强,但由于它们的小尺寸,很难测试疲劳.
- 现有的测量方法不足以评估单个CNT的疲劳行为.
研究的目的:
- 开发和实施一种用于评估单个碳纳米管 (CNT) 耐疲劳的新型测试系统.
- 在不同的条件下研究一厘米长的CNT的疲劳行为.
- 了解影响 CNT 疲劳寿命和断裂机制的因素.
主要方法:
- 开发一种非接触式声学共振测试系统.
- 应用该系统来测量单个CNT的疲劳行为
- 疲劳性质的分析,包括温度依赖和骨折的开始.
主要成果:
- CNT表现出了显著的耐疲劳性.
- CNTs的疲劳性能受到温度的显著影响.
- 在CNTs中疲劳骨折的时间主要取决于第一个缺陷的开始.
结论:
- 开发的非接触声响系统可以有效地测试单个CNT的疲劳.
- CNT具有出色的耐疲劳性,这是它们在结构应用中的关键属性.
- 了解缺陷的产生对于预测和提高CNT的疲劳寿命至关重要.
更多相关视频
09:47Facile Preparation of Internally Self-assembled Lipid Particles Stabilized by Carbon Nanotubes
Published on: February 19, 2016
10.0K
09:12Functionalization of Single-walled Carbon Nanotubes with Thermo-reversible Block Copolymers and Characterization by Small-angle Neutron Scattering
Published on: June 1, 2016
9.4K
相关概念视频
Network Covalent Solids
12.9K
Network covalent solids contain a three-dimensional network of covalently bonded atoms as found in the crystal structures of nonmetals like diamond, graphite, silicon, and some covalent compounds, such as silicon dioxide (sand) and silicon carbide (carborundum, the abrasive on sandpaper). Many minerals have networks of covalent bonds.
To break or to melt a covalent network solid, covalent bonds must be broken. Because covalent bonds are relatively strong, covalent network solids are typically...
To break or to melt a covalent network solid, covalent bonds must be broken. Because covalent bonds are relatively strong, covalent network solids are typically...
12.9K
Types Of Superconductors
1.7K
A superconductor is a substance that offers zero resistance to the electric current when it drops below a critical temperature. Zero resistance is not the only interesting phenomenon as materials reach their transition temperatures. A second effect is the exclusion of magnetic fields. This is known as the Meissner effect. A light, permanent magnet placed over a superconducting sample will levitate in a stable position above the superconductor. High-speed trains that levitate on strong...
1.7K
Abrasion Resistance of Concrete
833
Abrasion resistance is an essential characteristic of concrete that determines its durability and longevity under various wear conditions. Concrete surfaces are vulnerable to different types of abrasion. For instance, surfaces may wear down due to the constant movement of vehicles or be eroded by solids carried in water, as seen in concrete canal linings. Specific tests are conducted to measure the abrasion resistance of concrete.
One such test is the revolving disc test, where three plates...
One such test is the revolving disc test, where three plates...
833
Fiber Reinforced Concrete
645
Fiber-reinforced concrete significantly enhances the structural and nonstructural properties of traditional concrete by incorporating fibers like steel, glass, and polymers. These fibers, varying from natural ones such as sisal and cellulose to manufactured ones like polypropylene and Kevlar, are mixed into hydraulic cement with aggregates. Steel fibers, often preferred for their robustness, contribute to improved ductility, toughness, and post-cracking performance. The concrete is classified...
645
Mechanical Characteristics of Steel
942
The mechanical characteristics of steel are assessed through various tests that evaluate its strength, toughness, and flexibility. These tests include tension, torsion, impact, bending, and hardness assessments, each providing crucial information about steel's suitability for specific applications.
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...