不钢的局部腐蚀是由NaCl溶液中的典型含有物引起的:氧硫化物和MnS
Dan Li1, Hui Zhi1, Zhaogui Lai1
1National Center for Materials Service Safety, University of Science and Technology Beijing, Beijing 100083, China.
Materials (Basel, Switzerland)
|June 28, 2023
概括
不钢 (SS) 中的硫化 (MnS) 和氧硫化含量加速化溶液中的局部腐蚀. 这些含有物会产生电化学电位差异,增加对蚀的易受性.
科学领域:
- 材料科学 材料科学 材料科学
- 电化学 电化学 电化学
- 腐蚀科学 腐蚀科学
背景情况:
- 不钢 (SS) 的局部腐蚀是一种关键的故障机制.
- 硫化 (MnS) 和氧硫化含量在SS中很常见,并影响腐蚀行为.
- 了解这些含的电化学作用对于材料的耐用性至关重要.
研究的目的:
- 为了研究由MnS和氧硫化物含量诱导的SS的局部腐蚀行为.
- 为了阐明包含诱导腐蚀背后的电化学机制.
- 为了确定这些含有物对孔腐蚀易受性的影响.
主要方法:
- 在NaCl溶液中进行浸泡试验.
- 微电化学试验. 微电化学试验.
- 表面Volta电位测量. 表面Volta电位测量.
- 纳入成分和结构的分析.
主要成果:
- 氧硫化物含有物具有复杂的结构,具有明显的氧化物和硫化物相.
- 硫化物相比周围矩阵表现出较低的表面伏尔塔电位,类似于MnS.
- 含有MnS和氧硫化物都显著增加了不钢对局部蚀的易受性.
结论:
- 在不钢中,MnS和氧硫化物含有物是局部腐蚀的起始点.
- 包含组件的电化学电位差异和不同的溶解度会导致腐蚀.
- 控制包装特征对于提高SS对蚀的抗性至关重要.
更多相关视频
06:48Fluid-cell Raman Spectroscopy for operando Studies of Reaction and Transport Phenomena during Silicate Glass Corrosion
Published on: May 9, 2025
484
10:00Experimental Protocol to Determine the Chloride Threshold Value for Corrosion in Samples Taken from Reinforced Concrete Structures
Published on: August 31, 2017
15.5K
相关概念视频
Corrosion
25.2K
The degradation of metals due to natural electrochemical processes is known as corrosion. Rust formation on iron, tarnishing of silver, and the blue-green patina that develops on copper are examples of corrosion. Corrosion involves the oxidation of metals. Sometimes it is protective, such as the oxidation of copper or aluminum, wherein a protective layer of metal oxide or its derivatives forms on the surface, protecting the underlying metal from further oxidation. In other cases, corrosion is...
25.2K
Corrosion of Reinforcement
218
The corrosion of steel reinforcement within concrete is a process influenced by the material's inherent properties and external factors. The high pH level of around 13, provided by calcium hydroxide present in concrete, initially protects the steel reinforcement by promoting the formation of a passive iron oxide layer on its surface.
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
218
Formation of Complex Ions
23.8K
A type of Lewis acid-base chemistry involves the formation of a complex ion (or a coordination complex) comprising a central atom, typically a transition metal cation, surrounded by ions or molecules called ligands. These ligands can be neutral molecules like H2O or NH3, or ions such as CN− or OH−. Often, the ligands act as Lewis bases, donating a pair of electrons to the central atom. These types of Lewis acid-base reactions are examples of a broad subdiscipline called coordination...
23.8K
Qualitative Analysis
22.4K
For solutions containing mixtures of different cations, the identity of each cation can be determined by qualitative analysis. This technique involves a series of selective precipitations with different chemical reagents, each reaction producing a characteristic precipitate for a specific group of cations. Metal ions within a group are further separated by varying the pH, heating the mixture to redissolve a precipitate, or adding other reagents to form complex ions.
For instance, group IV...
For instance, group IV...
22.4K
Colloidal precipitates
629
The high insolubility of some precipitates can result in an unfavorable relative supersaturation. This can lead to colloidal particles with a large surface-to-mass ratio, where adsorption is promoted. For instance, in the precipitation of silver chloride, silver ions are adsorbed on the surface of the colloidal particles, forming a primary layer. This layer attracts ions of opposite charge (such as nitrate ions), forming a diffuse secondary layer of adsorbed ions. This electric double layer...
629
Sulfate Attack on Concrete
191
Sulfate attack on concrete is a deterioration process characterized by a whitish discoloration beginning at the edges and corners, accompanied by cracking and spalling. This phenomenon occurs when sulfates react with the components of hardened concrete, forming compounds like calcium sulfate and calcium sulfoaluminate which occupy more space than the substances they replace, causing the concrete to expand and disrupt.
Sulfates from sources like soil, groundwater, or industrial effluents...
Sulfates from sources like soil, groundwater, or industrial effluents...
191