预固化对纸质材料结构和性能的影响
Mingcen Lin1, Wenling Zhou1, Ye Yao1
1State Key Laboratory of Pulp and Paper Engineering, South China University of Technology, Guangzhou 510640, China.
Polymers
|June 28, 2023
概括
在热压之前引入预固化步骤显著改善了基于纸张的摩擦材料. 这种方法优化了树脂的分布,增强了机械性能,减少了变形,以获得更好的性能.
科学领域:
- 材料科学 材料科学 材料科学
- 机械工程 机械工程
背景情况:
- 传统的基于纸张的摩擦材料的热压导致树脂分布不均,并且由于压力效应而降低机械性能.
- 传统的固化过程没有充分考虑压力对复合材料中的矩阵树脂的影响.
研究的目的:
- 研究预固化方法对纸质摩擦材料表面形态和机械特性的影响.
- 优化预固化条件,以提高纸质摩擦材料的性能.
主要方法:
- 在热压阶段之前实施了预固化步骤.
- 该研究分析了不同级别的预固化对材料性能的影响.
- 在160°C10分钟内确定了最佳的预固化条件,达到60%的预固化程度.
主要成果:
- 预固化显著影响了树脂分布和界面粘合强度.
- 60%的预固化度允许树脂达到凝状态,保持孔隙结构并防止在热压时损坏.
- 优化的材料表现出增强的静态机械性能和减少永久变形.
结论:
- 提议的预固化方法有效地解决了传统热压纸质摩擦材料的限制.
- 达到特定的预固化程度 (60%) 对于平衡树脂分布,孔隙结构和机械完整性至关重要.
- 这种方法导致优越的静态和动态机械性能,使其成为摩擦材料技术的可行进步.
相关概念视频
Curing Methods
102
Concrete members with a small surface-to-volume ratio are cured by oiling and moistening the forms before casting the concrete member. These forms can be left in place for a prolonged period to prevent moisture loss, and can be wetted if made of a material suitable for wetting. If the forms are removed early, the concrete member is moistened and covered with polythene sheets to maintain moisture. For large horizontal concrete surfaces exposed to dry weather, a temporary covering is suspended...
102
Accelerated Curing of Concrete
192
Accelerating concrete curing is achieved by applying heat and additional moisture. This process accelerates the hydration of the cement, resulting in an earlier strength gain in the concrete. Steam curing is a method wherein the concrete products are either transported through a chamber on a conveyor belt or encased in plastic, allowing steam at atmospheric pressure to circulate freely around them. This process begins with a phase of moist curing that typically lasts between 3 to 5 hours, after...
192
Curing of Concrete
124
The hydration of cement takes place within the water-filled capillary pores. However, environmental elements can disrupt this process by evaporating water from the concrete surfaces. Sealed concrete with a water-cement ratio below 0.5 experiences self-desiccation, leading to water loss. The water loss in concrete is mitigated by curing. This technique involves keeping the concrete saturated to maintain the necessary temperature and moisture conditions, to optimally fill the spaces in the cement...
124