概括
对于Echelon10和Excelsior SL-10微导管,最佳的热炮成型需要使用120°C的温度30秒. 这种方法确保了成功的成型,即使是重复使用,而不会损坏SL-10微导管.
科学领域:
- 医疗器械 医疗器械
- 最少侵入性的手术
- 材料科学 材料科学 材料科学
背景情况:
- 微导管是最小侵入性手术中至关重要的工具.
- 精确的成型微导管对于导航复杂的血管系统至关重要.
- 热枪成型为定制微导管修改提供了一种方法.
研究的目的:
- 为了确定最佳的热枪温度和时间,以塑造Echelon10和Excelsior SL-10微导管.
- 在多次加热周期后评估成形微导管的耐用性和性能.
主要方法:
- 使用的是HAKKO FV-310热枪,温度设置为115°C和125°C.
- 微导管的形状采用了30,60和90秒的加热时间.
- 在距离热枪喷嘴2.5厘米处测量温度.
主要成果:
- 实际达到的温度分别为120.6°C和127.8°C,设置为115°C和125°C.
- Echelon10微导管在经过测试的温度和时间之间没有显著的形状差异.
- 卓越SL-10微导管在125°C时经历了尖端退化,需要使用115°C的设置.
结论:
- 在大约120°C的温度下,可以在30秒内成功塑造Echelon10和SL-10微导管的热枪.
- 温度为115°C,加热30秒,适合重复塑造微导管而不会发生退化.
- 温度超过130°C可能会导致退化,特别是在SL-10模型中.
相关概念视频
Heating and Cooling Curves
22.9K
When a substance—isolated from its environment—is subjected to heat changes, corresponding changes in temperature and phase of the substance is observed; this is graphically represented by heating and cooling curves.
For instance, the addition of heat raises the temperature of a solid; the amount of heat absorbed depends on the heat capacity of the solid (q = mcsolidΔT). According to thermochemistry, the relation between the amount of heat absorbed or released by a substance, q, and its...
For instance, the addition of heat raises the temperature of a solid; the amount of heat absorbed depends on the heat capacity of the solid (q = mcsolidΔT). According to thermochemistry, the relation between the amount of heat absorbed or released by a substance, q, and its...
22.9K
Accelerated Curing of Concrete
187
Accelerating concrete curing is achieved by applying heat and additional moisture. This process accelerates the hydration of the cement, resulting in an earlier strength gain in the concrete. Steam curing is a method wherein the concrete products are either transported through a chamber on a conveyor belt or encased in plastic, allowing steam at atmospheric pressure to circulate freely around them. This process begins with a phase of moist curing that typically lasts between 3 to 5 hours, after...
187