开发一种加速测试方法,以在加速条件下评估化真空绝缘板的长期热性能
Minjung Bae1,2, Sunsook Kim2, Jaesik Kang1
1Department of Building Energy Research, Korea Institute of Civil Engineering and Building Technology, Goyang 10223, Republic of Korea.
Materials (Basel, Switzerland)
|October 14, 2023
概括
一种新的加速测试方法显著缩短了蒸二氧化真空绝缘板 (VIP) 的评估时间. 这种方法只需70天就能准确预测长期的热性能,简化了VIP质量评估.
科学领域:
- 材料科学 材料科学 材料科学
- 热力工程是热力工程中的一个.
- 建筑科学 建筑科学
背景情况:
- 国际标准要求对真空绝缘板 (VIP) 的长期热性能进行长期的180天加速测试.
- 评估VIP的25年热性能对于建筑物的能源效率至关重要.
研究的目的:
- 开发一种简化,更快速的加快测试方法,用于化的VIP.
- 为了准确预测化VIP的长期热性能.
主要方法:
- 提出了一种高度加速的测试方法,使用80°C和70%的相对湿度 (RH).
- 与现有的加速方法 (50°C和70%RH) 进行比较.
- 分析了内部压力增速,并得出了长期导热率.
主要成果:
- 在高度加速的条件下70天后,内部压力增加率与加速条件下180天相匹配.
- 估计的长期导热率为0.0076 W/m·K (高度加速) 和0.0054 W/m·K (加速).
- 拟议的方法允许大约70天的条件条件可用于可靠的评估.
结论:
- 开发的高度加速方法提供了显著更快的评估化VIP的长期热性能.
- 这种简化方法可以有效地生产具有一致热性质的VIP.
- 在80°C和70%RH下的70天测试是国际标准评估的可行替代方案.
更多相关视频
07:48Artificial Thermal Ageing of Polyester Reinforced and Polyvinyl Chloride Coated Technical Fabric
Published on: January 29, 2020
6.6K
07:15A Testing Platform for Durability Studies of Polymers and Fiber-reinforced Polymer Composites under Concurrent Hygrothermo-mechanical Stimuli
Published on: December 11, 2014
13.8K
相关概念视频
Thermal Insulation in Masonry Walls
128
In hot, dry climates, the thermal mass of masonry walls can be beneficial, absorbing heat during the day and releasing it at night, thereby stabilizing indoor temperatures. However, in most other climates, additional insulation is necessary to enhance thermal resistance.
External insulation can be applied using an Exterior Insulation and Finish System (EIFS), which involves affixing panels of plastic foam to the wall and covering them with a polymeric stucco reinforced with glass fiber mesh....
External insulation can be applied using an Exterior Insulation and Finish System (EIFS), which involves affixing panels of plastic foam to the wall and covering them with a polymeric stucco reinforced with glass fiber mesh....
128
Soundness of Cement
192
The soundness of cement refers to the ability of cement paste to retain its volume after setting. Unsound cement can lead to expansion and structural damage due to the presence of free lime, magnesia, and calcium sulfate. Free lime hydrates very slowly, expanding and causing unsoundness, which is difficult to detect because it intercrystallizes with other compounds. Magnesia also reacts with water, forming crystals that can disrupt the cement's structure. Calcium sulfate can create...
192