煤炭暴露于酸性矿井排水 (AMD) 的孔隙和分子结构演化的机制
Jin-Zhi Luo1, Yan-Yan Cai2, Hao Tang3
1School of Civil Engineering, Fujian Research Center for Tunneling and Urban Underground Space Engineering, Huaqiao University, Xiamen, Fujian 361021, China; Key Laboratory of Geological Support for Coal Green Exploitation, Xi'an, Shaanxi 710054, China.
The Science of the total environment
|October 16, 2023
概括
酸性矿井排水 (AMD) 通过改变孔隙结构和分子组成,显著降低了煤炭的特性. 这项研究揭示了AMD如何增加孔隙性和透性,影响废弃矿山的安全性.
科学领域:
- 地质化学 地质化学
- 材料科学 材料科学 材料科学
- 环境科学 环境科学
背景情况:
- 酸性矿井排水 (AMD) 对已退役的煤矿构成重大风险,特别是在富含硫的煤炭地区.
- 了解因AMD而导致的煤炭恶化的机制对于矿山安全和环境管理至关重要.
研究的目的:
- 调查煤炭特性恶化的微观结构和分子机制,这是由于长时间暴露在酸性矿井排水 (AMD) 引起的.
- 阐明AMD酸度的变化如何影响煤炭的孔隙性,透性和宏分子结构.
主要方法:
- 煤样品经过2到5的pH范围的浸泡测试.
- 使用了微观方法,包括计算机断层扫描 (CT),核磁共振 (NMR),扫描电子显微镜 (SEM) 和里埃变换红外光谱 (FTIR).
主要成果:
- 暴露于AMD导致孔隙和裂扩散的增加,特别是在煤层,严重程度与AMD酸度相关.
- 在严重的AMD条件下,NMR和SEM表明从微孔转向宏孔,并增加了孔的大小,从而提高了煤炭的透性.
- FTIR分析证实了AMD在降解煤炭大分子和增加矩阵层孔隙性方面的作用.
结论:
- AMD显著改变了煤炭的孔隙结构和分子完整性,增加了透性并导致结构降解.
- 这些发现为管理AMD影响的废弃煤矿的安全和环境影响提供了关键的见解.
相关概念视频
Acid Attack on Concrete
223
When acids come into contact with concrete, they initiate a chemical reaction that dissolves the hydrated cement paste. This process leads to softening and structural weakening of the concrete. This issue is commonly observed in environments such as chimneys, sewers, and industrial settings. The severity of the damage increases as the pH of the water interacting with the concrete drops below 6.5. In particular, a pH under 4.5 can cause significant concrete damage.
The rate at which hydrogen...
The rate at which hydrogen...
223
Pore Size Distribution
143
In concrete, the pore size distribution significantly influences the material's properties. Capillary pores, markedly larger than gel pores, form a vast network within partially hydrated cement paste, reducing the concrete's strength and increasing its permeability. This heightened permeability leads to a greater risk of damage from environmental factors like freeze-thaw cycles and chemical attacks, with the extent of vulnerability also being tied to the water-to-cement ratio.
Adequate...
Adequate...
143
Porosity and Absorption of Aggregate
300
Aggregates contain pores of varying sizes; while some are completely enclosed within the particles, others open onto the surface, allowing water to penetrate. The porosity of aggregates is a major factor contributing to the overall porosity of concrete, given that aggregates constitute about three-quarters of concrete's volume.
When all pores in an aggregate are filled with water, the aggregate is considered saturated and surface-dry. If left in dry air, water will evaporate until the...
When all pores in an aggregate are filled with water, the aggregate is considered saturated and surface-dry. If left in dry air, water will evaporate until the...
300
Acid Strength and Molecular Structure
30.9K
Binary Acids and Bases
In the absence of any leveling effect, the acid strength of binary compounds of hydrogen with nonmetals (A) increases as the H-A bond strength decreases down a group in the periodic table. For group 17, the order of increasing acidity is HF < HCl < HBr < HI. Likewise, for group 16, the order of increasing acid strength is H2O < H2S < H2Se < H2Te. Across a row in the periodic table, the acid strength of binary hydrogen compounds increases with...
In the absence of any leveling effect, the acid strength of binary compounds of hydrogen with nonmetals (A) increases as the H-A bond strength decreases down a group in the periodic table. For group 17, the order of increasing acidity is HF < HCl < HBr < HI. Likewise, for group 16, the order of increasing acid strength is H2O < H2S < H2Se < H2Te. Across a row in the periodic table, the acid strength of binary hydrogen compounds increases with...
30.9K
Molecular Structure and Acidity
17.3K
An acid can be deprotonated to form a conjugate base or an anion. If the produced anion is more stable, then the acid is stronger. On the contrary, if the anion is unstable, then the acid is weaker. Hence, to determine the acidity of the compound, the stability of its conjugate base is studied using various factors.
The size effect explains the change in atomic size on acidity. When comparing the acids formed from elements that belong to the same column in the periodic table, their atomic sizes...
The size effect explains the change in atomic size on acidity. When comparing the acids formed from elements that belong to the same column in the periodic table, their atomic sizes...
17.3K
Porosity in Cement Paste
151
The porosity of concrete is a measure of the void spaces within its structure. These spaces impact its strength and durability significantly. When water and cement interact, a chemical reaction called hydration creates a semi-solid paste. This paste includes combined water, making up approximately 23% of the cement's dry mass, and gel water, which fills minuscule voids known as gel pores, accounting for about 28% of the cement gel volume.
The balance of water to cement in the mix is...
The balance of water to cement in the mix is...
151