合成条件和工艺参数对气凝特性的影响
Ozge Payanda Konuk1, Ala A A M Alsuhile2, Hamed Yousefzadeh3
1Department of Materials Science and Engineering, Koç University, Istanbul, Türkiye.
Frontiers in chemistry
|November 8, 2023
概括
本综述探讨了合成条件和工艺参数如何影响气凝特性. 了解这些因素是定制纳米孔材料以适应吸附和绝缘等特定应用的关键.
科学领域:
- 材料科学 材料科学 材料科学
- 纳米技术 纳米技术
- 化学工程是化学工程的重要组成部分.
背景情况:
- 气凝是先进的纳米孔质材料,具有特殊的特性,如低密度和高表面积.
- 它们的调节性特性源于各种前体 (无机,有机,混合) 和合成方法.
- 主要应用包括吸附,隔热,催化,组织工程和药物输送.
研究的目的:
- 提供综合条件和工艺参数的综合审查,以量身定制气凝的特性.
- 研究各种合成阶段对气凝特性的影响.
- 为了突出控制合成与应用特定性能之间的联系.
主要方法:
- 关于空气凝合成的已发表研究的文献综述.
- 从前体溶解到超临界干燥的参数分析.
- 包括碳气凝的碳化工艺.
主要成果:
- 确定了影响气凝性质的关键合成参数.
- 证明了工艺控制对孔隙结构和材料特性的影响.
- 强调了为特定应用量身定制合成的重要性.
结论:
- 合成条件和工艺参数对于控制气凝特性至关重要.
- 量身定制的气凝合成可用于各种应用的优化.
- 对合成步骤的精确控制的进一步研究可以解锁新的材料功能.
相关概念视频
Precipitation Processes
The experimental conditions in a gravimetric analysis should be optimized to maximize the particle size and purity of the obtained precipitate. Ideally, the concentration of the precipitating reagent should be low with effective stirring to maintain low relative supersaturation for the growth of large crystals. In homogeneous precipitation, the precipitant is slowly generated by a chemical reaction in the solution to avoid local reagent excesses. For example, urea decomposes gradually to...
Factors Affecting Workability
The workability of concrete is a critical characteristic that influences the ease of mixing, handling, and finishing the concrete. It is affected by several factors including water content, aggregate properties, and admixtures like air entrainment. Water plays a fundamental role as it lubricates the concrete mix, facilitating easier movement and placement. However, the water requirement varies depending on the texture and shape of aggregates. Finer particles and angular, rough-textured...
Carbonation Shrinkage
Atmospheric CO2 penetrates the concrete's pores and, in the presence of moisture, forms carbonic acid, which then reacts with calcium hydroxide in the hydrated cement, forming calcium carbonate. This process reduces the concrete's volume and is termed carbonation shrinkage.
The concrete's permeability is slightly reduced as calcium carbonate produced during the reaction fills its pores. Furthermore, its strength is slightly enhanced as the water released during the reaction facilitates the...
The concrete's permeability is slightly reduced as calcium carbonate produced during the reaction fills its pores. Furthermore, its strength is slightly enhanced as the water released during the reaction facilitates the...
Air-entraining Agents
Air-entraining agents improve the durability and workability of concrete in climates with frequent freezing and thawing. These agents prevent cracks by introducing small air bubbles into the mix, creating spaces accommodating water expansion when temperatures drop. The air-entraining agents lower the surface tension of water, forming stable, small air bubbles. This method is more effective than having accidental large voids, as the intentional, smaller, and evenly distributed air voids improve...
Effects of Air-entrainment in Concrete
Air entrainment in concrete significantly enhances the material's durability, especially in environments subjected to freeze-thaw cycles. Introducing small air bubbles into the concrete mix acts as internal voids that accommodate the expansion of water when it freezes, thereby alleviating internal stress and preventing structural cracks. This function is crucial in climates with significant freezing and thawing, as it protects the concrete from repeated stresses that could lead to premature...
Turbulent Flow: Problem Solving
Carbonation is a process used to dissolve carbon dioxide gas in a liquid, commonly used in the production of carbonated beverages. Achieving efficient carbonation requires careful control of temperature, pressure, and flow conditions. By adjusting these parameters, carbonation efficiency can be maximized, producing a higher concentration of CO2 in the liquid.
Temperature is a key factor in CO2 solubility. In this case, the CO2 gas and the liquid are cooled to 20°C. Lower temperatures enhance...
Temperature is a key factor in CO2 solubility. In this case, the CO2 gas and the liquid are cooled to 20°C. Lower temperatures enhance...