基于统计混合设计方法的PG-FA-L复合修饰剂的配方,用于修复广的土壤
Fusheng Zha1, ChuanQing Hu1, Bo Kang1
1School of Resource and Environmental Engineering, Hefei University of Technology, Hefei, 230009, China.
Chemosphere
|December 20, 2023
概括
这项研究引入了一个复合修改系统 (PG-FA-L) 扩张性土壤,显著改善其性能. 该系统增强土壤强度,控制土壤膨胀,为地质工程应用提供了可行的解决方案.
科学领域:
- 地质技术工程 地质技术工程
- 材料科学 材料科学 材料科学
- 环境科学 环境科学
背景情况:
- 广的土壤在土木工程项目中带来了重大挑战.
- 用单一的固体废物材料修改广的土壤可以获得低于最佳的结果.
- 对有问题的土壤需要先进的稳定技术.
研究的目的:
- 调查复合材料修改系统 (PG-FA-L) 的有效性,以改善扩张性土壤特性.
- 评估单个成分 (PG,FA,L) 对土壤强度和膨胀行为的影响.
- 为了确定路床填充应用的复合材料系统的最佳剂量.
主要方法:
- 用PG-FA-L系统处理广土壤的实验分析.
- 统计分析以评估房地产改进.
- 在28天后评估不受限制的压力强度和变形特性.
- 对火山灰反应动力学的分析.
主要成果:
- 该PG-FA-L系统显著提高了固化膨胀土壤的整体特性.
- 波特兰水泥 (PG) 和飞灰 (FA) 提高了土壤强度超过特定的门;石灰 (L) 在所有阶段都提高了强度.
- 石灰 (L) 显著减少了土壤的膨胀,但过量产生了负面影响.
- 波特兰水泥 (PG) 加快了火山灰的反应.
结论:
- 使用PG-FA-L系统的复合修改为广的土壤提供了一种优越的方法,而不是单元修改.
- 优化的PG,FA和L剂量可以有效地改善土壤强度,并控制道路施工的胀.
- 这种方法为在土壤稳定中利用固体废物提供了可持续的解决方案.
相关概念视频
Design Example: Managing Concrete Workability
81
This example deals with managing the workability of concrete for a raft foundation project under hot weather conditions. Workability is crucial for ensuring the concrete is easy to place, compact, and finish. In this scenario, a slump test — a common method to measure the workability of fresh concrete — initially indicated low workability. This was attributed to the rapid water loss from the concrete mix, exacerbated by the high temperatures causing the course aggregates to heat up.
81
Design Example: Aggregate Gradation
94
The right type and quality of aggregates are crucial for concrete as they significantly influence its properties, mix proportions, and cost-effectiveness. If different sources are available for sand, the commonly used fine aggregate in concrete, the selection of sand is primarily based on its gradation.
The grading, or particle-size distribution, of sand is determined using sieve analysis, with standard sizes ranging from 150 μm to 10 mm (ASTM No. 100 sieve to 3⁄8 in. sieve). Sand is...
The grading, or particle-size distribution, of sand is determined using sieve analysis, with standard sizes ranging from 150 μm to 10 mm (ASTM No. 100 sieve to 3⁄8 in. sieve). Sand is...
94
Compacting Factor test
163
The compacting factor test is a method used to assess the workability of concrete. It is especially suitable for concrete mixes containing aggregates up to one and a half inches in size. This test involves specialized equipment consisting of two truncated cone-shaped hoppers and a cylinder, all with polished interior surfaces to minimize friction.
The procedure begins by placing concrete into the upper hopper without any compaction. Once filled, the bottom door of this hopper is opened,...
The procedure begins by placing concrete into the upper hopper without any compaction. Once filled, the bottom door of this hopper is opened,...
163
Method of Superposition
869
The method of superposition is a crucial technique in structural engineering, used to analyze the effect of multiple loads on beams. This approach involves calculating the deflection and slope for each load on a beam separately, and then summing these effects to determine the overall impact. It is applicable only when the beam material remains within its elastic limit, ensuring that deformations are linearly elastic.
When applying the method of superposition, each type of load—whether...
When applying the method of superposition, each type of load—whether...
869
Factors Affecting Workability
72
The workability of concrete is a critical characteristic that influences the ease of mixing, handling, and finishing the concrete. It is affected by several factors including water content, aggregate properties, and admixtures like air entrainment. Water plays a fundamental role as it lubricates the concrete mix, facilitating easier movement and placement. However, the water requirement varies depending on the texture and shape of aggregates. Finer particles and angular, rough-textured...
72
Superplasticizers
85
Superplasticizers are advanced admixtures that enhance the workability of concrete by lowering the water content without compromising the strength of the material. These substances are highly effective water reducers, improving concrete flow, making it easier to work with, and enabling concrete to reach inaccessible areas or densely reinforced sections without mechanical vibration. The key components in superplasticizers are either sulfonated melamine or naphthalene formaldehyde condensates,...
85