基于支向量机的混凝土振动状态的图像识别和参数分析
Shuai Wang1, Aixun Wang2, Xudong Fu3
1Wuhan University; Wuhan Construction Engineering Group Co. Ltd.; 356797825@qq.com.
Journal of visualized experiments : JoVE
|January 22, 2024
概括
这项研究表明,定向梯度直方图和支向量机 (SVM) 技术可以准确地识别混凝土的振动状态. 优化参数在混凝土振动分析中实现了100%的识别准确性.
科学领域:
- 材料科学 材料科学 材料科学
- 土木工程 土木工程是指土木工程.
- 计算机视觉 计算机视觉
背景情况:
- 监测混凝土的完整性对于结构安全至关重要.
- 由于复杂的特征提取,在振动下评估混凝土具有挑战性.
研究的目的:
- 评估使用定向梯度直方图和SVM用于混凝土振动状态识别的可行性.
- 分析方向梯度直方图参数对识别精度的影响.
主要方法:
- 使用定向梯度直方图谱技术从具体图像中提取特征.
- 使用支向量机 (SVM) 模型对振动状态进行分类.
- 对识别准确度的参数灵敏度 (块大小,统计间隔,二元化值) 的分析.
主要成果:
- 定向梯度直方图-SVM技术可用于混凝土振动状态识别.
- 识别精度对方向梯度直方图参数敏感,具有最佳范围.
- 通过优化参数和高分辨率图像 (1024x1024像素) 实现了100%的识别精度.
结论:
- 拟议的方法为非破坏性混凝土状况监测提供了一种可行的方法.
- 参数优化是最大限度地提高定向梯度直方图-SVM技术的性能的关键.
- 这种技术有可能在结构健康监测中得到实际应用.
相关概念视频
Vibrating Concrete
99
Mechanical vibrators are instrumental in compacting newly poured concrete within formwork and around reinforcements. This process is essential to eliminate trapped air pockets and establish a dense concrete mass. One widely used method is vibrating by internal vibrators, often referred to as a poker vibrator or immersion vibrator. It is rapidly inserted through the full depth of the freshly laid concrete and slightly extends into the layer below it (which remains in a plastic state). Consistent...
99
Dynamic Modulus of Elasticity of Concrete
348
The dynamic modulus of elasticity assesses how a concrete structure deforms under impact or dynamic loads. It is typically higher than the static modulus of elasticity, measured under slow, steady loading conditions.
The sonic test is a common method to determine the dynamic modulus. In this test, a concrete beam, sized either 6 x 6 x 30 inches or 4 x 4 x 20 inches, is clamped at its center. Vibrations are initiated at one end of the beam by an electromagnetic exciter unit powered by...
The sonic test is a common method to determine the dynamic modulus. In this test, a concrete beam, sized either 6 x 6 x 30 inches or 4 x 4 x 20 inches, is clamped at its center. Vibrations are initiated at one end of the beam by an electromagnetic exciter unit powered by...
348
Vebe Test
146
The Vebe test is a method used to measure the workability of concrete, particularly effective for dry concrete mixes. This test employs a specific apparatus that includes a cylindrical chamber, a standard slump cone, and a transparent disc-shaped rider, all mounted on a vibrating table. The cylindrical chamber has dimensions of nine and a half inches in diameter and eight inches in height.
To conduct the test, concrete is placed into the slump cone. The concrete is filled in layers and...
To conduct the test, concrete is placed into the slump cone. The concrete is filled in layers and...
146
Segregation in Fresh Concrete
132
Segregation in fresh concrete is a phenomenon where the components of the concrete mix separate, leading to uneven distribution and compromised structural integrity. This separation typically occurs when concrete is subjected to excessive horizontal movement within forms, or when it is dropped from considerable heights or forced through narrow, winding paths. As a result, heavier coarse aggregate particles settle at the bottom, while lighter, finer materials such as cement and water rise to the...
132
Abrasion Resistance of Concrete
134
Abrasion resistance is an essential characteristic of concrete that determines its durability and longevity under various wear conditions. Concrete surfaces are vulnerable to different types of abrasion. For instance, surfaces may wear down due to the constant movement of vehicles or be eroded by solids carried in water, as seen in concrete canal linings. Specific tests are conducted to measure the abrasion resistance of concrete.
One such test is the revolving disc test, where three plates...
One such test is the revolving disc test, where three plates...
134
Microcracking in Concrete
122
Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
122