一个初级牙的应力分布与不钢皇冠恢复使用不同的化水泥
Mehmet Sami Guler1, Cigdem Guler2, Nihal Belduz Kara2
1Department of Machinery and Metal Technologies, Vocational School of Technical Sciences, Ordu University, Ordu, Turkey.
BMC oral health
|February 23, 2024
概括
在初级上,不钢皇冠 (SSC) 经历了树脂水泥比玻璃离子体水泥更高的应力. 玻璃离子体水泥可以减少儿科SSC修复中的压力,防止化水泥骨折.
科学领域:
- 生物材料科学 生物材料科学
- 牙科材料 牙科材料
- 机械工程 机械工程
背景情况:
- 用不钢皇冠 (SSC) 恢复的初级牙在儿科牙科中很常见.
- 选择水泥可以影响这些修复的机械行为和寿命.
研究的目的:
- 为了评估和比较用SSC修复的初级牙的应力分布,使用不同的化水泥.
- 用有限元素分析 (FEA) 分析树脂和玻璃离子体水泥对模拟咬伤力下的应力度的影响.
主要方法:
- 从DICOM数据创建了一个具有SSC的初级的3D有限元模型.
- 两个化水泥 (自愈合粘合树脂水泥和玻璃离子体水泥) 用30微米层模拟.
- 应用了330N的垂直和斜负荷来模拟最大的咬伤力.
主要成果:
- 所有模型的最大Von Mises应力值在施加力和闭合接触区域是最高的.
- 与玻璃离子体水泥 (220.06 MPa 垂直, 198.72 MPa 斜) 相比,使用树脂水泥的SSC模型的最大应力 (478.09 MPa 垂直, 214.62 MPa 斜) 显著更高.
结论:
- 如果压力超过其耐力极限,高咬伤力可能导致化水泥骨折.
- 使用玻璃离子体水泥用于初级牙的SSC修复,可以有效地降低压力水平,从而有可能改善儿童的修复耐用性.
相关概念视频
Stress Concentrations
287
Stress concentration is when stress intensifies near discontinuities such as holes or abrupt cross-sectional changes in a structural member. This localized stress can often surpass the average stress within the member. The stress distribution in flat bars, either with a circular hole or varying widths connected by fillets, can be determined experimentally using a photoelastic method. The results are based on ratios of geometric parameters like the ratio of the hole's radius to the smaller...
287
Residual Stresses
220
Residual stresses reside in a structure even after removing the original stress inducer. This phenomenon often arises from varied plastic deformations across different parts of a structure. Consider a rod stretched beyond its yield point. It will not regain its original length due to permanent deformation. Even after load removal, the rod does not entirely lose stress because of uneven plastic deformations, resulting in residual stresses. The computation of these stresses in structures is...
220
Porosity in Cement Paste
135
The porosity of concrete is a measure of the void spaces within its structure. These spaces impact its strength and durability significantly. When water and cement interact, a chemical reaction called hydration creates a semi-solid paste. This paste includes combined water, making up approximately 23% of the cement's dry mass, and gel water, which fills minuscule voids known as gel pores, accounting for about 28% of the cement gel volume.
The balance of water to cement in the mix is...
The balance of water to cement in the mix is...
135