对微观结构,组成和加载条件对Mg合金应力腐蚀裂变行为的影响进行数据分析

Jianan Gu1, D C Florian Wieland1, Domonkos Tolnai1

  • 1Institute of Metallic Biomaterials, Helmholtz-Zentrum Hereon, Max-Planck Str.1, 21502 Geesthacht, Germany.

概括

稀土合金中的应力腐蚀裂变 (SCC) 是一个重大挑战. 本研究分析了文献数据,以开发Mg-Gd合金的预测性SCC模型,确定二次相含量作为关键因素.

相关概念视频

Stress Concentrations01:24

Stress Concentrations

Stress concentration is when stress intensifies near discontinuities such as holes or abrupt cross-sectional changes in a structural member. This localized stress can often surpass the average stress within the member. The stress distribution in flat bars, either with a circular hole or varying widths connected by fillets, can be determined experimentally using a photoelastic method. The results are based on ratios of geometric parameters like the ratio of the hole's radius to the smaller...
286
Fatigue01:21

Fatigue

Fatigue occurs when materials rupture under repeated or fluctuating loads, even at stress levels far below their static breaking strength. It typically results in brittle failure, even for ductile materials. It is a critical consideration in designing machines and structural components subjected to repetitive or varying loads. The nature of these loadings can range from fluctuating loads like unbalanced pump impellers causing vibrations to repeatedly bending a thin steel rod wire back and forth...
181
Microcracking in Concrete01:20

Microcracking in Concrete

Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
117
Relation between Poisson's ratio, Modulus of Elasticity and Modulus of Rigidity01:15

Relation between Poisson's ratio, Modulus of Elasticity and Modulus of Rigidity

Deformation occurs in axial and transverse directions when an axial load is applied to a slender bar. This deformation impacts the cubic element within the bar, transforming it into either a rectangular parallelepiped or a rhombus, contingent on its orientation. This transformation process induces shearing strain. Axial loading elicits both shearing and normal strains. Applying an axial load instigates equal normal and shearing stresses on elements oriented at a 45° angle to the load axis.
264
Stress: General Loading Conditions01:15

Stress: General Loading Conditions

To grasp the intricacy of real-world conditions where multiple loads are applied simultaneously to a structure, one might visualize a section passing through a specific point within a body, aligned parallel to the xy plane. This section is subjected to various forces, including original loads, normal forces, and shearing forces.
The shearing force, possessing potential directionality within the plane of the section, is simplified into two component forces running parallel to the x and y axes....
307
Stress-Strain Diagram - Ductile Materials01:24

Stress-Strain Diagram - Ductile Materials

The stress-strain relationship in ductile materials such as structural steel or aluminium is intricate and progresses through several stages. When a specimen is loaded, it initially exhibits a linear length increase, depicted by a steep straight line on the stress-strain diagram. It indicates the material is elastically deforming and will return to its original shape once unloaded. However, when a critical stress value is reached, plastic deformation begins. This stage sees substantial...
709