概括
回收玻璃的质量下降,影响其实际的原材料替代. 我们的模型仅显示了83%的有效替代,由于质量损失,回收收益减少了13-23%
科学领域:
- 环境科学 环境科学
- 材料科学 材料科学 材料科学
- 废物管理 废物管理
背景情况:
- 废物管理的可持续性评估需要工具来评估回收过程中的材料质量退化.
- 现有的研究主要集中在塑料上,而其他材料 (如玻璃) 的模型存在差距.
- 玻璃的可回收性往往被高估,忽略了污染和颜色等因素,导致不准确的生命周期评估 (LCA) 假设.
研究的目的:
- 开发和评估玻璃废物的可替代性模型.
- 测量新材料和回收碎玻璃 (cullet) 之间的替代程度.
- 将技术质量和市场适用性纳入玻璃回收的影响评估中.
主要方法:
- 根据技术质量 (杂质,颜色) 和市场需求,制定了玻璃的可替代性模型.
- 将模型应用于关于玻璃废物处理的欧洲案例研究.
- 我们比较了两种情景:完全替代与将质量下降考虑在内的替代.
主要成果:
- 考虑到质量下降,只有83%的碎片有效地取代了原材料.
- 在考虑质量损失时,玻璃回收的好处在不同影响类别中减少了13-23% .
- 这与完全一对一替代的假设形成鲜明对比.
结论:
- 质量恶化对玻璃回收的实际好处产生重大影响.
- 开发的模型提供了对玻璃回收可持续性的更准确的评估.
- 未来的LCA应纳入材料质量退化,以进行现实的废物管理评估.
相关概念视频
Design Example: Aggregate Gradation
93
The right type and quality of aggregates are crucial for concrete as they significantly influence its properties, mix proportions, and cost-effectiveness. If different sources are available for sand, the commonly used fine aggregate in concrete, the selection of sand is primarily based on its gradation.
The grading, or particle-size distribution, of sand is determined using sieve analysis, with standard sizes ranging from 150 μm to 10 mm (ASTM No. 100 sieve to 3⁄8 in. sieve). Sand is...
The grading, or particle-size distribution, of sand is determined using sieve analysis, with standard sizes ranging from 150 μm to 10 mm (ASTM No. 100 sieve to 3⁄8 in. sieve). Sand is...
93
Deleterious Substances in Aggregate
166
Deleterious substances in aggregates can be detrimental to the quality and durability of concrete. These substances include organic impurities like loam, which interfere with cement hydration and are usually present in the sand. These prevent a good bond between aggregate and cement paste. Organic impurities can be detected using the colorimetric test, where the darkness of a solution after agitation indicates the level of organic content.
Another type of impurity is clay and fine material that...
Another type of impurity is clay and fine material that...
166
Plasticity
2.1K
Plasticity is the property where an object loses its elasticity and undergoes irreversible deformation, even after the deformation forces are eliminated. If a material deforms irreversibly without increasing stress or load, then this is called ideal plasticity. For example, when a force is applied to an aluminum rod, it changes its shape, but it does not return to its original shape once the force is removed. Plastic deformation or ductility is thus a permanent deformation or change in the...
2.1K
Unsoundness of Aggregate due to Volume Change
106
Unsoundness in aggregates due to volume changes is primarily caused by the physical alterations aggregates undergo, such as freezing and thawing, thermal changes, and wetting and drying. Unsound aggregates, when subjected to these changes, result in volume change upon disintegration. This, in turn, contributes to the deterioration of concrete, including scaling, pop-outs, and cracking. Particular types of aggregates, such as porous flints, cherts, and those containing clay minerals, are...
106