Zhongxiang Liu1, Tong Guo2, Wenjie Li3

  • 1School of Transportation, Southeast University, Nanjing 210096, China.

PubMed
概括

-合金涂层显著提高桥梁电缆线的耐用性,防止腐蚀疲劳. 这项研究显示,Zn-Al涂层提供了卓越的保护,将使用寿命延长了约29.1年.

相关概念视频

Cable Subjected to a Distributed Load01:24

Cable Subjected to a Distributed Load

The analysis of suspension bridges is a complex and critical process that involves multiple factors, including the shape and tension of the main cables. The main cables of suspension bridges are subjected to distributed loads, which result in changes in tensile forces and deformation of the cable. These loads must be carefully considered to ensure that the bridge is safe and capable of supporting the weight of different loads.
679
Fatigue01:21

Fatigue

Fatigue occurs when materials rupture under repeated or fluctuating loads, even at stress levels far below their static breaking strength. It typically results in brittle failure, even for ductile materials. It is a critical consideration in designing machines and structural components subjected to repetitive or varying loads. The nature of these loadings can range from fluctuating loads like unbalanced pump impellers causing vibrations to repeatedly bending a thin steel rod wire back and forth...
181
Cable Subjected to Concentrated Loads01:28

Cable Subjected to Concentrated Loads

Flexible cables are commonly used in various applications for support and load transmission. Consider a cable fixed at two points and subjected to multiple vertically concentrated loads. Determine the shape of the cable and the tension in each portion of the cable, given the horizontal distances between the loads and supports.
822
Cable: Problem Solving01:29

Cable: Problem Solving

When dealing with a cable that is fixed to two supports and subjected to uniform loading, it is crucial to determine the maximum tension in the cable. This process can be broken down into several key steps, as outlined below:
327
Cable Subjected to Its Own Weight01:13

Cable Subjected to Its Own Weight

Overhead power transmission lines rely on cables to carry electricity across large distances. To ensure the stability and functionality of these lines, it is crucial to understand the shape and tension experienced by the cables under the influence of their weight.
A generalized loading function is employed to analyze a cable subjected to its own weight. This function considers the force acting along the cable's arc length rather than its projected length, providing a more accurate...
450
Fatigue Strength of Concrete01:22

Fatigue Strength of Concrete

Fatigue, in the context of materials science and engineering, refers to the weakening or failure of a material caused by repeatedly applied loads, even if these loads are below the strength limit of the material. Fatigue strength in concrete is a critical property that influences its durability and longevity. Concrete can fail in two ways due to fatigue. Static fatigue or creep rupture occurs under a constant load or one that increases slowly. The other failure mode is due to cyclical or...