在植入物上沉积的原子层沉积改善了骨中的骨质整合

Hong-Joo Kim1, Seon-Ki Lee2, Hyun-Seung Kim3

  • 1Department of Prosthodontics, School of Dentistry, Chonnam National University, Gwangju, Republic of Korea.

概括

的原子层沉积 (ALD) 增强了植入物的骨质整合. 涂有的植入物在体内改善了骨形成和骨与植入物接触,这表明植入物成功率更高.

相关概念视频

Bone Remodeling01:40

Bone Remodeling

Bone remodeling is a continuous and balanced process of bone resorption by osteoclasts and bone formation by osteoblasts. In adults, it helps maintain bone mass and calcium homeostasis. While mechanical stress can stimulate turnover as part of the normal maintenance and reparative process, several hormones also regulate bone remodeling.
Osteoclasts in Bone Remodeling01:31

Osteoclasts in Bone Remodeling

Osteoclasts are cells responsible for bone resorption and remodeling. They originate from hematopoietic progenitor cells present in the bone marrow. Numerous progenitor cells fuse to form multinucleated cells, each with 10-20 nuclei. A single osteoclast has a diameter of 150 to 200 µM. These cells have ruffled borders that break down the underlying bone tissue and release minerals such as calcium into the blood in bone resorption. Osteoclasts cling to bones with their ruffled edges during bone...
The Bone Matrix01:18

The Bone Matrix

Bone contains a relatively small number of cells entrenched in a matrix of collagen fibers that provide an adherent surface for inorganic salt crystals. Both components of the matrix, organic and inorganic, contribute to the unusual properties of bone. Without collagen, bones would be brittle and shatter easily. Without mineral crystals, bones would flex and provide little support. This can be observed by an experiment: when the minerals of a bone are dissolved by soaking the bone in acid or...
Bone Formation by Intramembranous Ossification01:29

Bone Formation by Intramembranous Ossification

Intramembranous ossification is one of the two processes involved in the development of bones within an embryo. The flat bones of the face, most of the cranial bones, and the clavicles are formed via this process. During intramembranous ossification, the bones develop directly from sheets of undifferentiated mesenchymal connective tissue.
The process begins when mesenchymal cells in the embryonic skeleton gather together and differentiate into osteogenic cells, which then develop into...
Essential Minerals for Bone Health01:31

Essential Minerals for Bone Health

The minerals contained in all of the food we consume are essential for our organ systems. However, certain essential minerals, such as calcium, phosphorus, magnesium, manganese, and fluoride, largely affect bone health.
Calcium and Phosphorus
Calcium is a critical component of bones, especially in the form of calcium phosphate and calcium carbonate. Since the body cannot make calcium, it must be obtained from the diet. However, calcium cannot be absorbed from the small intestine without...
Bone Formation by Endochondral Ossification01:24

Bone Formation by Endochondral Ossification

Bone formation, or ossification, begins around the sixth to seventh week of embryonic development. Most bones develop from a cartilaginous template through the process of endochondral ossification. Cartilage formation begins when clusters of mesenchymal cells differentiate into chondrocytes. These chondrocytes proliferate rapidly and secrete an extracellular matrix that becomes encased in a membrane called the perichondrium. The resulting cartilage model provides a template that resembles the...