在聚合物改性青混凝土混合物中使用粉碎底灰作为填充剂来提高可持续性和性能
Yeong-Min Kim1, Kyungnam Kim2, Tri Ho Minh Le3
1Department of Highway & Transportation Research, Korea Institute of Civil Engineering and Building Technology, 283 Goyangdae-Ro, Ilsanseo-Gu, Goyang-si 10223, Gyeonggi-do, Republic of Korea.
Polymers
|June 27, 2024
概括
这项研究发现,在青混凝土混合物中用25%的粉碎底灰取代石灰填充剂可以显著提高路面性能. 这种可持续的方法提高了青路面的耐用性,防腐蚀性和防潮性.
科学领域:
- 土木工程 土木工程是指土木工程.
- 材料科学 材料科学 材料科学
- 环境工程 环境工程
背景情况:
- 对可持续建筑材料的需求不断增长.
- 需要将回收材料纳入路面工程中的必要性.
- 作为建筑填充剂的工业副产品的探索.
研究的目的:
- 评估使用压碎的热电厂底灰作为聚合物改性青混凝土中的填充物.
- 为了确定传统的石灰填充剂的底层灰的最佳替代水平.
- 评估底层灰对青混合物性能的影响.
主要方法:
- 底层灰在0%,25%,50%和75%的水平上取代了石灰填充剂.
- 使用间接抗拉强度 (ITS),动态模量,坎塔布罗,汉堡轮跟踪 (HWT) 和抗拉强度比 (TSR) 测试进行性能评估.
- 对照混合物的比较与最佳的25%底灰修饰混合物.
主要成果:
- 根据ITS测试,确定最佳替代水平为25%.
- 25%的底灰混合物显示出增强的道耐用性 (HWT测试中7.56毫米与8.9毫米).
- 观察到更好的磨损耐力,更高的刚性和更好的耐湿性 (更高的TSR).
结论:
- 25%的粉碎底灰是聚合物改性青混凝土的可行填充物.
- 底灰增强了青混合物密度,粘合剂-聚合物粘合力和整体耐用性.
- 这为改善路面性能和寿命提供了一个可持续的解决方案.
相关概念视频
Additives and Fillers in Concrete
93
Additives and fillers are integral to enhancing the properties of concrete. Pozzolans and blast-furnace slag are additives or admixtures due to their reactions with calcium hydroxide released during cement hydration. Fillers, which are finely ground and similar in fineness to Portland cement, improve concrete attributes such as workability density, and reduce capillary bleeding or cracking. Some fillers possess hydraulic properties or participate in benign reactions within the cement paste.
The...
The...
93
Pozzolans
110
Pozzolans are siliceous or aluminous materials blended with Portland cement. They interact with the calcium hydroxide produced during the hydration of Portland cement and contribute to improved strength and durability of concrete. The pozzolanic activity, a measure of a pozzolan's effectiveness, is typically assessed using the strength activity index, as defined in ASTM C 618-93, which calculates the ratio of the compressive strength of cement mixtures with and without pozzolan.
Fly ash is...
Fly ash is...
110
Fiber Reinforced Concrete
74
Fiber-reinforced concrete significantly enhances the structural and nonstructural properties of traditional concrete by incorporating fibers like steel, glass, and polymers. These fibers, varying from natural ones such as sisal and cellulose to manufactured ones like polypropylene and Kevlar, are mixed into hydraulic cement with aggregates. Steel fibers, often preferred for their robustness, contribute to improved ductility, toughness, and post-cracking performance. The concrete is classified...
74
Superplasticizers
81
Superplasticizers are advanced admixtures that enhance the workability of concrete by lowering the water content without compromising the strength of the material. These substances are highly effective water reducers, improving concrete flow, making it easier to work with, and enabling concrete to reach inaccessible areas or densely reinforced sections without mechanical vibration. The key components in superplasticizers are either sulfonated melamine or naphthalene formaldehyde condensates,...
81
Effects of Air-entrainment in Concrete
82
Air entrainment in concrete significantly enhances the material's durability, especially in environments subjected to freeze-thaw cycles. Introducing small air bubbles into the concrete mix acts as internal voids that accommodate the expansion of water when it freezes, thereby alleviating internal stress and preventing structural cracks. This function is crucial in climates with significant freezing and thawing, as it protects the concrete from repeated stresses that could lead to premature...
82
Deleterious Substances in Aggregate
162
Deleterious substances in aggregates can be detrimental to the quality and durability of concrete. These substances include organic impurities like loam, which interfere with cement hydration and are usually present in the sand. These prevent a good bond between aggregate and cement paste. Organic impurities can be detected using the colorimetric test, where the darkness of a solution after agitation indicates the level of organic content.
Another type of impurity is clay and fine material that...
Another type of impurity is clay and fine material that...
162