概括
选择三酸密封剂和封闭技术显著影响根管孔隙性. 用单形和热垂直方法的EndoSequence BC显示出较少的顶端毛孔,而使用这些技术的NeoSealer Flo显示出较少的冠状毛孔.
科学领域:
- 牙周内科医院 牙周内科医院 牙周内科医院
- 牙科材料科学 牙科材料科学
- 生物材料是一种生物材料.
背景情况:
- 根管密封剂对于成功的内牙治疗至关重要.
- 根管填充物中的多孔性可能会损害治疗结果.
- 基于三酸盐的密封剂在密封能力方面具有潜在的优势.
研究的目的:
- 为了比较两个三酸密封剂的多孔性:EndoSequence BC和NeoSealer Flo.
- 评估三种堵塞技术 (单形,热垂直,冷侧面) 对密封器多孔性的影响.
- 用微型CT来评估单根牙的顶峰和冠状区域的密封体多孔性.
主要方法:
- 通过EndoSequence BC或NeoSealer Flo和gutta-percha.六个单根人类牙被堵塞.
- 使用单形,热垂直或冷侧面技术进行了遮.
- 通过X射线微型计算机断层扫描 (微型CT) 和深度学习细分,分析了顶峰和冠状区域的多孔性.
主要成果:
- 与NeoSealer Flo. BC相比,EndoSequence BC在单形和热垂直技术的应用中呈现出较低的孔隙性.
- 与EndoSequence BC.相比,NeoSealer Flo使用单形和热垂直技术在冠状动脉上表现出较低的孔隙性.
- 在这两个地区,在使用冷侧面技术的密封器之间没有观察到显著的孔径差异.
结论:
- 选择酸密封剂和堵塞技术对于最大限度地减少多孔性至关重要.
- 不同的密封剂-技术组合在顶端和冠状根运河三分之一中产生不同水平的多孔性.
- 优化密封剂和技术选择可以提高根管堵塞的质量.
更多相关视频
06:16Author Spotlight: Establishing an Accurate Microhardness Testing Protocol for Craniofacial Tissues
Published on: April 26, 2024
668
07:42Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
353
相关概念视频
Porosity in Cement Paste
122
The porosity of concrete is a measure of the void spaces within its structure. These spaces impact its strength and durability significantly. When water and cement interact, a chemical reaction called hydration creates a semi-solid paste. This paste includes combined water, making up approximately 23% of the cement's dry mass, and gel water, which fills minuscule voids known as gel pores, accounting for about 28% of the cement gel volume.
The balance of water to cement in the mix is...
The balance of water to cement in the mix is...
122
Porosity and Absorption of Aggregate
275
Aggregates contain pores of varying sizes; while some are completely enclosed within the particles, others open onto the surface, allowing water to penetrate. The porosity of aggregates is a major factor contributing to the overall porosity of concrete, given that aggregates constitute about three-quarters of concrete's volume.
When all pores in an aggregate are filled with water, the aggregate is considered saturated and surface-dry. If left in dry air, water will evaporate until the...
When all pores in an aggregate are filled with water, the aggregate is considered saturated and surface-dry. If left in dry air, water will evaporate until the...
275
Microcracking in Concrete
115
Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
115
Pore Size Distribution
114
In concrete, the pore size distribution significantly influences the material's properties. Capillary pores, markedly larger than gel pores, form a vast network within partially hydrated cement paste, reducing the concrete's strength and increasing its permeability. This heightened permeability leads to a greater risk of damage from environmental factors like freeze-thaw cycles and chemical attacks, with the extent of vulnerability also being tied to the water-to-cement ratio.
Adequate...
Adequate...
114