概括
铜90/10合金在受污染的海水中由于不受保护的膜而遭受加速腐蚀. 含有高营养素的污染场所造成的物质损失比自然海水更大.
科学领域:
- 材料科学 材料科学 材料科学
- 腐蚀工程 腐蚀工程
- 海洋学 海洋学 海洋学
背景情况:
- 铜合金提供出色的水性耐腐蚀性.
- 然而,污染或水的海水可能会导致加速腐蚀和过早失效.
- 这种行为可能源于早期暴露期间不受保护的腐蚀膜形成.
研究的目的:
- 研究铜90/10合金中的腐蚀现象.
- 在两个不同的阿拉伯海海水组成中比较腐蚀.
- 分析海洋热交换器管道的过早故障.
主要方法:
- 暴露在天然和污染的海水中,长达150天.
- 使用减重和维度计量技术测量腐蚀损失.
- 研究失败的海洋热交换器管.
- 使用SEM,EDS,XRD和拉曼散射来描述腐蚀沉积物.
主要成果:
- 在富含污染物和营养物质的污染海水区域观察到显著更高的腐蚀损失.
- 与天然海水中的优惠券相比,腐蚀率更高.
- 失败的热交换器管道表现出类似的腐蚀模式.
结论:
- 污染的海水,特别是含有大量溶解无机化合物的地方,显著加快了铜90/10合金的腐蚀.
- 了解早期腐蚀膜的形成对于防止海洋环境中过早失效至关重要.
- 这些发现强调了需要选择材料和运营策略,考虑到特定的海水质量.
更多相关视频
07:12Determining Tribocorrosion Rate and Wear-Corrosion Synergy of Bulk and Thin Film Aluminum Alloys
Published on: September 11, 2018
11.3K
12:18Co-localizing Kelvin Probe Force Microscopy with Other Microscopies and Spectroscopies: Selected Applications in Corrosion Characterization of Alloys
Published on: June 27, 2022
2.6K
相关概念视频
Testing Water Quality
634
When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
634
Effect of Sea Water on Concrete
1.4K
Concrete exposed to seawater can undergo degradation like the dissolution of ettringite and gypsum, increasing the material's porosity and decreasing its strength. In contrast, the crystallization of salts within the concrete's pores can cause expansion, particularly above the waterline where evaporation occurs. Nonetheless, this expansion only happens when seawater, enabled by the concrete's permeability, manages to infiltrate the structure.
Concrete in areas between tide marks,...
Concrete in areas between tide marks,...
1.4K