基和基替代的:合成和研究作为潜在的原子层沉积前体

Majeda Al Hareri1, Patricio Romero2, James F Britten3

  • 1Department of Chemistry, McMaster University, 1280 Main St. West, Hamilton, Ontario L8S 4M1, Canada.

Inorganic chemistry
|October 21, 2024
PubMed
概括

合成了新的含分子,具有重的基或基组. 这些化合物显示为元素的原子层沉积 (ALD) 的前体,为薄膜制造提供了一条新的途径.

相关概念视频

Hydroboration-Oxidation of Alkenes03:08

Hydroboration-Oxidation of Alkenes

In addition to the oxymercuration–demercuration method, which converts the alkenes to alcohols with Markovnikov orientation, a complementary hydroboration-oxidation method yields the anti-Markovnikov product. The hydroboration reaction, discovered in 1959 by H.C. Brown, involves the addition of a B–H bond of borane to an alkene giving an organoborane intermediate. The oxidation of this intermediate with basic hydrogen peroxide forms an alcohol.
7.9K
Preparation and Reactions of Sulfides02:26

Preparation and Reactions of Sulfides

Sulfides are the sulfur analog of ethers, just as thiols are the sulfur analog of alcohol. Like ethers, sulfides also consist of two hydrocarbon groups bonded to the central sulfur atom. Depending upon the type of groups present, sulfides can be symmetrical or asymmetrical. Symmetrical sulfides can be prepared via an SN2 reaction between 2 equivalents of an alkyl halide and one equivalent of sodium sulfide.
4.7K
Alkynes to Aldehydes and Ketones: Hydroboration-Oxidation02:47

Alkynes to Aldehydes and Ketones: Hydroboration-Oxidation

Introduction
One of the convenient methods for the preparation of aldehydes and ketones is via hydration of alkynes. Hydroboration-oxidation of alkynes is an indirect hydration reaction in which an alkyne is treated with borane followed by oxidation with alkaline peroxide to form an enol that rapidly converts into an aldehyde or a ketone. Terminal alkynes form aldehydes, whereas internal alkynes give ketones as the final product.
17.8K
Preparation of Alcohols via Addition Reactions02:15

Preparation of Alcohols via Addition Reactions

Overview
The acid-catalyzed addition of water to the double bond of alkenes is a large-scale industrial method used to synthesize low-molecular-weight alcohols. An acidic atmosphere is required to allow the hydrogen in the water molecule to act as an electrophile and attack the double bond in an alkene. The addition of a proton to the double bond creates a carbocation intermediate. The proton preferentially bonds to the less substituted end of the double bond to create a more stable carbocation...
6.1K
Diazonium Group Substitution with Halogens and Cyanide: Sandmeyer and Schiemann Reactions01:20

Diazonium Group Substitution with Halogens and Cyanide: Sandmeyer and Schiemann Reactions

Arenediazonium substitution reactions occur when the diazonium group is substituted by various functional groups such as halides, hydroxyl, nitrile, etc. For instance, arenediazonium salts react with copper(I) salts of chloride, bromide, or cyanide to form corresponding aryl chlorides, bromides, and nitriles. These reactions are named Sandmeyer reactions. Although the mechanism of this reaction is complicated, as illustrated in Figure 1, they are believed to progress via an aryl copper...
1.9K
Hybridization of Atomic Orbitals I03:24

Hybridization of Atomic Orbitals I

The mathematical expression known as the wave function, ψ, contains information about each orbital and the wavelike properties of electrons in an isolated atom. When atoms are bound together in a molecule, the wave functions combine to produce new mathematical descriptions that have different shapes. This process of combining the wave functions for atomic orbitals is called hybridization and is mathematically accomplished by the linear combination of atomic orbitals. The new orbitals that...
46.6K