一个老化的金属玻璃结构的结构复原
Yang Gao1,2, Cheng Yang1,2, Gan Ding1,3
1State Key Laboratory of Nonlinear Mechanics, Institute of Mechanics, Chinese Academy of Sciences, Beijing 100190, China.
Fundamental research
|October 21, 2024
概括
金属玻璃的再生方式不同于预期. 基于Zr的金属玻璃通过无弹性变形再生,由玻色子热容量峰值表明,而不是外热变化. 这表明了对玻璃再生机制的新理解.
科学领域:
- 材料科学 材料科学 材料科学
- 凝聚物质物理学 凝聚物质物理学
- 物理化学 物理化学
背景情况:
- 玻璃再生通常与玻璃过渡之前的外热变化有关.
- 了解金属玻璃中的再生机制对于其应用和稳定性至关重要.
研究的目的:
- 为了研究一个严重老化的Zr基金属玻璃中的复苏过程.
- 为了确定玻璃再生的替代指标,超出传统的度测量.
主要方法:
- 无弹性变形和热容量的实验分析.
- 潜在能源景观的特征和原子自由体积的重新分配.
- 调查稳定流状态和固有的结构.
主要成果:
- 基于Zr的金属玻璃在屈服之前通过无弹性变形再生,偏离了典型的外热热行为.
- 通过低温玻色子热容量峰值和有效度变化,可以准确地检测出复原.
- 该过程涉及降低机械稳定性而不会改变潜在能源景观盆地的能量水平,由原子自由体积再分配驱动.
结论:
- 玻璃再生可以通过降低机械稳定性而不是改变能量水平来发生.
- 玻色子峰作为一个更有效的探测器,与力相比,在眼镜中进行结构复原.
- 稳定流状态代表了再生的极限,其特点是具有自我相似的固有结构.
相关概念视频
Metallic Solids
21.5K
Metallic solids such as crystals of copper, aluminum, and iron are formed by metal atoms. The structure of metallic crystals is often described as a uniform distribution of atomic nuclei within a “sea” of delocalized electrons. The atoms within such a metallic solid are held together by a unique force known as metallic bonding that gives rise to many useful and varied bulk properties.
All metallic solids exhibit high thermal and electrical conductivity, metallic luster, and...
All metallic solids exhibit high thermal and electrical conductivity, metallic luster, and...
21.5K
The Effect of Aging on Tissues
4.2K
Several body functions deteriorate with age. The external signs of aging are easily identifiable. For example, the skin becomes dry, less elastic, and thins out, forming wrinkles. The skin of the face begins to appear looser due to a decrease in the levels of elastic and collagen fibers in the connective tissue. Additionally, melanin production in the hair follicle decreases with age, resulting in gray hair. Moreover, the senses of sight and hearing decline, so glasses and hearing aids may...
4.2K
Corrosion of Reinforcement
726
The corrosion of steel reinforcement within concrete is a process influenced by the material's inherent properties and external factors. The high pH level of around 13, provided by calcium hydroxide present in concrete, initially protects the steel reinforcement by promoting the formation of a passive iron oxide layer on its surface.
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
726