在深埋的岩层中基于泥泥和岩石之间的合效应进行纵向裂解和接
Liu Xiangyang1,2, Cheng Hua3,4, Xu Xueqing5
1School of Urban Construction and Transportation, Hefei University, Hefei, 230041, Anhui, China. lxymm9632@163.com.
Scientific reports
|December 3, 2024
概括
这项研究模拟了破碎岩石中粘土分裂的模型,发现初始高粘土压力和速度是泥扩散的关键. 后来,增加泥粘度对于有效的断裂密封至关重要.
科学领域:
- 地质技术工程 地质技术工程
- 土木工程 土木工程是指土木工程.
- 材料科学 材料科学 材料科学
背景情况:
- 泥岩合效应会影响断裂通道宽度和接压力.
- 这种效应随着泥扩散而减少,远离接孔.
研究的目的:
- 为泥岩合建立一个纵向料分裂模型.
- 分析泥运动和断裂扩张动态.
主要方法:
- 导出了一个分离泥的扩散运动方程.
- 集成的时间变化的泥粘度和断裂宽度减弱.
主要成果:
- 最初,低泥粘度意味着接压力和速率决定了扩散范围.
- 超过粘度值后,粘度成为主要的扩散限制因素.
- 最佳的接策略涉及高的初始速率/压力,其次是增加密封的粘度.
结论:
- 接参数必须适应泥粘度的变化.
- 有效的断裂密封需要对泥特性和注入参数采取动态方法.
相关概念视频
Placing Concrete
80
The concrete is placed as close as possible to its final position to avoid segregation. The placed concrete is then fully compacted to expel the entrapped air, and the next layer of concrete is laid while the underlying layer is still in the plastic state. The rate at which concrete is placed and compacted is kept equal.
While placing concrete, care is taken to ensure that the concrete is laid in uniform layers, and hand shoveling and moving concrete using poker vibrators is avoided. Also,...
While placing concrete, care is taken to ensure that the concrete is laid in uniform layers, and hand shoveling and moving concrete using poker vibrators is avoided. Also,...
80
Types of Building Separation Joints
192
Building separation joints divide large or complex building structures into smaller, discrete units that can move independently. These joints are categorized into three types: volume-change joints, settlement joints, and seismic separation joints.
Volume-change joints address the effects of expansion and contraction due to temperature and moisture variations. They are strategically placed at discontinuities in a building's mass where cracking is most likely and are spaced about 150 to 200...
Volume-change joints address the effects of expansion and contraction due to temperature and moisture variations. They are strategically placed at discontinuities in a building's mass where cracking is most likely and are spaced about 150 to 200...
192
Shrinkage in Concrete
79
Shrinkage in concrete is primarily due to water loss from evaporation, hydration of cement, or carbonation, leading to a reduction in volume. The volumetric contraction results in volumetric strain in concrete. However, in practice, shrinkage is measured as linear strain, which is one-third of the volumetric strain.
When concrete is still in its plastic state, it can undergo a decrease in volume by about 1% of its absolute volume. This decrease is known as plastic shrinkage. It arises either...
When concrete is still in its plastic state, it can undergo a decrease in volume by about 1% of its absolute volume. This decrease is known as plastic shrinkage. It arises either...
79
Preplaced Aggregate Concrete
92
Preplaced aggregate concrete is ideal for construction environments that are not easily accessible. The process begins by properly wetting the gap-graded coarse aggregates to remove the dirt, then placing it in the form and compacting it. Voids are filled with a mortar mix pumped under pressure through slotted pipes. This mortar typically consists of Portland cement, pozzolan, fine aggregates, water, and a fluidizing aid. The pozzolan helps reduce bleeding and segregation while improving the...
92
Porosity in Cement Paste
116
The porosity of concrete is a measure of the void spaces within its structure. These spaces impact its strength and durability significantly. When water and cement interact, a chemical reaction called hydration creates a semi-solid paste. This paste includes combined water, making up approximately 23% of the cement's dry mass, and gel water, which fills minuscule voids known as gel pores, accounting for about 28% of the cement gel volume.
The balance of water to cement in the mix is...
The balance of water to cement in the mix is...
116
Slump Test
143
The slump test is a widely used method to measure the workability of concrete. It employs a 12-inch high truncated cone mold that tapers from eight inches at the base to four inches at the top. Before testing, the mold is securely attached to a flat base and dampened.
Concrete is poured into the mold in three layers to conduct the test. Each layer is compacted 25 times with a steel tamping rod, which has a five-eighths-inch diameter and a rounded end, to ensure even distribution and eliminate...
Concrete is poured into the mold in three layers to conduct the test. Each layer is compacted 25 times with a steel tamping rod, which has a five-eighths-inch diameter and a rounded end, to ensure even distribution and eliminate...
143