使用基于漂移比率的碎形维度对弹性混凝土柱的定量地震损害评估
Bunka Son1, Ganggang Li2, Zhiwei Luo1
1Graduate School of System Informatics, Kobe University, 1-1 Rokkodai-cho, Nada, Kobe 657-8501, Japan.
Materials (Basel, Switzerland)
|December 17, 2024
概括
本研究引入了碎形维度 (FD) 分析,以量化性混凝土柱中的地震损害. 碎形维度有效地表明损坏水平,并与结构性能指标相关联,有助于修复性评估.
科学领域:
- 土木工程 土木工程是指土木工程.
- 结构工程 结构工程
- 材料科学 材料科学 材料科学
背景情况:
- 坚固的混凝土柱子对于地震易发地区的地震安全至关重要.
- 需要对地震损害进行准确的定量评估,才能制定有效的修复和改造战略.
研究的目的:
- 开发和验证耐震混凝土柱的定量地震损害评估模型.
- 建立裂纹图案的碎形维度 (FD) 和结构性能指标之间的关系.
主要方法:
- 使用盒子计数算法进行碎形分析,从裂纹模式中推导出FD.
- 在反向循环负荷下对八个混凝土柱进行实验测试.
- 在FD,短暂漂移比率,残余漂移比率和相对刚性损失 (RSL) 之间的相关性分析.
主要成果:
- 碎形维度 (FD) 是一个高效的,基于图像的指标,用于确定混凝土柱的地震损伤.
- FD与短暂漂移比率有很强的相关性,并受剪切跨度比率的影响.
- 开发了线性和多线性方程,将FD与漂移比率和RSL用于损害评估.
结论:
- 拟议的基于FD的模型提供了一种可靠的方法,用于对弹性混凝土柱的定量地震损害评估.
- 飞行器设计为评估结构可修复性和整体损坏程度提供了一种有价值的工具,它补充了现有的设计指南.
更多相关视频
相关概念视频
Dynamic Modulus of Elasticity of Concrete
254
The dynamic modulus of elasticity assesses how a concrete structure deforms under impact or dynamic loads. It is typically higher than the static modulus of elasticity, measured under slow, steady loading conditions.
The sonic test is a common method to determine the dynamic modulus. In this test, a concrete beam, sized either 6 x 6 x 30 inches or 4 x 4 x 20 inches, is clamped at its center. Vibrations are initiated at one end of the beam by an electromagnetic exciter unit powered by...
The sonic test is a common method to determine the dynamic modulus. In this test, a concrete beam, sized either 6 x 6 x 30 inches or 4 x 4 x 20 inches, is clamped at its center. Vibrations are initiated at one end of the beam by an electromagnetic exciter unit powered by...
254
Design of Columns under a Centric Load
104
The design of columns under centric load is a fundamental aspect of structural engineering and is critical for ensuring the stability and integrity of structures. Euler's and Secant's formulas are central to understanding and calculating the critical load and deformation behaviors of columns, providing a basis for safe and effective structural design.
Euler's formula is applicable under the assumption that the column is a perfect, straight, homogenous prism, and it is operating...
Euler's formula is applicable under the assumption that the column is a perfect, straight, homogenous prism, and it is operating...
104
Elasticity in Concrete
82
Upon subjecting concrete to moderate or high uniaxial compressive or tensile stresses, the strain response is non-linear relative to the stress applied. As the stress is removed, the resulting stress-strain curve deviates from the original path traced during loading, creating a hysteresis loop, indicative of the concrete's non-linear and non-elastic properties. Typically, a material's modulus of elasticity, which is a measure of the material's stiffness, is inferred from the linear...
82
Effects of Creep
89
Creep in concrete, the gradual deformation under prolonged stress, significantly impacts the integrity of structures. For reinforced concrete beams, it can be a vital design consideration, as it increases deflection, sometimes necessitating additional design measures. In columns, especially slender ones under eccentric loads, creep can cause buckling, compromising their stability. However, creep can be beneficial in indeterminate structures by mitigating stresses that arise from shrinkage,...
89
Design of Columns under an Eccentric Load
437
Designing columns to withstand eccentric loads is a critical aspect of structural engineering, ensuring structures can support off-center loads without failure. This design process must account for the additional normal stresses introduced by eccentric loading, which can significantly influence a column's stress distribution and overall stability. An eccentric load applied to a column induces normal stresses that can be conceptualized as a combination of stresses due to an equivalent...
437
Microcracking in Concrete
100
Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
100