优化多晶钻石紧位的选择和钻井参数,用于偏差井在伊拉克Majnoon领域,伊拉克
Ahmed N Al-Dujaili1, Maaly S Asad2, Najah Saeed3
1Petroleum Engineering Department, Amirkabir University of Technology, No. 350, Hafez Ave, Valiasr Square, Tehran, 1591634311, Iran. ahmed.noori203@aut.ac.ir.
Scientific reports
|January 25, 2025
概括
在Majnoon Field优化钻探参数和比特选择显著减少了钻探问题. 特定的位型和钻井轨迹,如J形,提高了透率和稳定性.
科学领域:
- 石油工程是石油工程中的一个.
- 钻井优化 钻井优化
- 井口建设工程 井口建设工程
背景情况:
- 钻井操作面临诸多挑战,包括钻孔磨损和漏洞清洁不良.
- 优化钻探参数对于效率和成本效益至关重要.
研究的目的:
- 优化比特选择和钻探参数,以提高Majnoon领域的性能.
- 确定垂直和偏斜井的最有效的钻井方法.
主要方法:
- 分析伊拉克东南部的Majnoon田的钻探数据.
- 评估不同的钻头类型 (SFD75D,MMD,MME,FX,EQ) 及其性能.
- 钻井参数的评估:比特重量 (WOB),RPM,泥重量和流量.
- 钻井轨迹的比较 (J形与S形) 以及它们对钻井效率的影响.
主要成果:
- 16英寸SFD75D位显示出优越的定向能力,用于垂直和偏离井.
- 在12.25英寸和8.5英寸的截面上,MMD和MME比特表现优于FX和EQ类型.
- 确定了最佳的钻井参数:WOB (25.45-73 klbs),RPM (50-179.22),泥重量 (10.5-10.8 ppg) 和流量 (662-940 gpm).
- 与S型井相比,J型井的透率增加了50-100%,扭矩更稳定.
- 南方井表现出较高的滑动百分比,但比北方井更稳定的倾斜和较低的液压要求.
结论:
- 比特选择和参数优化是缓解钻井问题和增强孔清洁的关键.
- 建议使用SFD75D,MMD和MME位用于Majnoon领域的特定部分.
- J形井轨迹在钻井性能和稳定性方面具有显著的优势.
相关概念视频
Quarrying of Stone
Quarrying is the process of extracting stone from a quarry, where specialized techniques are employed to remove large blocks of stone safely and efficiently. This process can involve controlled explosions or more precision-oriented methods such as cutting and drilling.
One common method involves using a diamond belt saw to cut large blocks from the quarry face. These blocks can be about 50 feet long and 12 feet high. After the initial vertical cut, drilling is performed at the base of the block.
One common method involves using a diamond belt saw to cut large blocks from the quarry face. These blocks can be about 50 feet long and 12 feet high. After the initial vertical cut, drilling is performed at the base of the block.
Microcracking in Concrete
Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...