压电牙科缩放器对两个不同的可浮复合材料填充材料的粗性影响
1Faculty of Dentistry, Department of Periodontology, Marmara University; o_birkan@yahoo.com.
Journal of visualized experiments : JoVE
|January 29, 2025
概括
牙科超声波缩放器显著增加可流动复合材料的表面粗度,可能导致更多的斑块积累和牙周病. 这一发现影响了修复性牙科实践.
科学领域:
- 牙科材料科学 牙科材料科学
- 牙周病学 牙周病学
- 生物材料工程 生物材料工程
背景情况:
- 牙科超声波缩放器对于牙周治疗至关重要.
- 牙修复的表面粗性可以促进斑块的积累,这是牙周病的主要因素.
研究的目的:
- 为了评估压电超声波缩放器对两个不同的可流动复合材料表面粗度的影响.
- 评估使用缩放器对复合材料修复完整性和斑块保留的潜在临床影响.
主要方法:
- 使用了两种类型的可流动复合材料,每种10个圆盘形样本.
- 在应用超声波缩放器之前和之后,使用形计和扫描电子显微镜分析了表面粗度.
- 缩放器应用涉及标准化参数:60s 持续时间,水冷却和调节力.
主要成果:
- 剖面测量显示,在缩放器应用后,两种复合材料的表面粗度显著增加 (p < 0.01).
- 扫描电子显微镜证实了表面粗度的定性增加.
- 两种复合材料之间没有观察到初始或后缩放器表面粗度的显著差异 (分别为p = 0.143和p = 0.684).
结论:
- 高功率的压电超声波缩放器可以在可流动复合材料修复中诱导大量的表面粗.
- 这种诱导的粗性可能会增加斑块积累的风险,可能会危及牙周健康.
- 纳米混合体流动复合材料与传统的单体可能会在使用超声波缩放器时表现出类似的表面变化.
更多相关视频
07:42Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
303
03:37Impact of Fabrication Techniques and Polishing Procedures on Surface Roughness of Denture Base Resins
Published on: January 17, 2025
260
相关概念视频
Strength of Cement
926
Strength tests for cement are not performed directly on neat cement paste due to difficulty in obtaining consistent, reliable specimens. Instead, cement is typically tested in the form of cement-sand mortar.
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
926
Superplasticizers
477
Superplasticizers are advanced admixtures that enhance the workability of concrete by lowering the water content without compromising the strength of the material. These substances are highly effective water reducers, improving concrete flow, making it easier to work with, and enabling concrete to reach inaccessible areas or densely reinforced sections without mechanical vibration. The key components in superplasticizers are either sulfonated melamine or naphthalene formaldehyde condensates,...
477
Additives and Fillers in Concrete
500
Additives and fillers are integral to enhancing the properties of concrete. Pozzolans and blast-furnace slag are additives or admixtures due to their reactions with calcium hydroxide released during cement hydration. Fillers, which are finely ground and similar in fineness to Portland cement, improve concrete attributes such as workability density, and reduce capillary bleeding or cracking. Some fillers possess hydraulic properties or participate in benign reactions within the cement paste.
The...
The...
500