在冷却用水供应系统中对形,腐蚀和生物污染进行全面评估
Olha Biedunkova1, Pavlo Kuznietsov1, Oleg Pinchuk1
1National University of Water and Environmental Engineering, 33028 Rivne, Ukraine.
MethodsX
|February 3, 2025
概括
一种新方法结合了直接和间接的监测,以评估冷却水系统的腐蚀,规模和生物污染. 这种方法提高了核电站运营的可靠性和安全性.
科学领域:
- 水处理 处理水的方法
- 腐蚀科学 腐蚀科学
- 环境微生物学 环境微生物学
背景情况:
- 核电站的冷却水系统 (CWS) 对于安全运行至关重要.
- 传统的监测方法往往无法提供全面评估CWS健康状况.
- 腐蚀,形和生物污染对CWS的效率和安全构成重大风险.
研究的目的:
- 开发和验证核电站冷却水系统的综合监测方法.
- 整合直接和间接的评估技术进行整体的评估.
- 提高对废燃料储存设施的监测效率.
主要方法:
- 间接方法:兰吉尔和指数 (LSI),瑞斯纳尔稳定指数 (RSI),pH,温度,总溶解盐,总硬度,总度.
- 直接方法:腐蚀速率 (V),形速率 (S) 通过实验室测试.
- 生物评估:酵母和细菌的殖民地形成单位 (CFU),藻类细胞计数,水箱水分析.
主要成果:
- 综合方法提供了对耐腐蚀性和形潜力的同时评估.
- 通过CFU,藻类计数和水箱评估实现了详细的生物污染分析.
- 与传统方法相比,增强的监测技术提供了对CWS条件的更全面的了解.
结论:
- 经过验证的方法使得核电站冷却水系统的预测风险建模成为可能.
- 可以实施优化策略,以确保核电站运行的可靠性和安全性.
- 这种全面的方法解决了关键基础设施现有监控实践的局限性.
相关概念视频
Precipitation and Co-precipitation
1.7K
Precipitation and coprecipitation methods can be used to separate a mixture of ions in a solution. In qualitative inorganic analysis, ions that form sparingly soluble precipitates with the same reagent are separated based on the differences in solubility products. For example, consider the separation of Cu(II) and Fe(II) ions by precipitation as insoluble sulfides. First, copper(II) sulfide is precipitated by the addition of acidic H2S, where the dissociation of H2S is suppressed. Adding H2S...
1.7K
Corrosion of Reinforcement
156
The corrosion of steel reinforcement within concrete is a process influenced by the material's inherent properties and external factors. The high pH level of around 13, provided by calcium hydroxide present in concrete, initially protects the steel reinforcement by promoting the formation of a passive iron oxide layer on its surface.
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
156
Coagulation
258
Colloidal solids are solid particles suspended in solution. They are usually negatively charged, attracting a compact primary layer of positively charged ions, which attract more counterions to form an electrical double layer. Electrostatic repulsion between the charged double layers prevents the particles from colliding, stabilizing the colloids. These solids are often undesirable because they can contain toxins that are difficult to remove. Coagulation is a technique that helps aggregate and...
258
Multiple Pipe Systems
388
Multipipe systems consist of complex configurations of interconnected pipes designed to transport fluids efficiently across intricate networks. They are essential in engineering applications requiring precise control over flow distribution, pressure, and head loss. They are categorized into series, parallel, loop, and network configurations, each distinguished by unique flow characteristics and applications.
Series Configuration
In a series configuration, fluid flows sequentially from one pipe...
Series Configuration
In a series configuration, fluid flows sequentially from one pipe...
388
Corrosion
23.6K
The degradation of metals due to natural electrochemical processes is known as corrosion. Rust formation on iron, tarnishing of silver, and the blue-green patina that develops on copper are examples of corrosion. Corrosion involves the oxidation of metals. Sometimes it is protective, such as the oxidation of copper or aluminum, wherein a protective layer of metal oxide or its derivatives forms on the surface, protecting the underlying metal from further oxidation. In other cases, corrosion is...
23.6K