相关实验视频
Updated: May 27, 2025

06:58
Zinc-Sponge Battery Electrodes that Suppress Dendrites
Published on: September 29, 2020
4.3K
无机金属混合涂层用于稳定和调节水性阳极
Jinliang Li1, Yao Dai1, Qian Chen1
1School of Materials Science and Engineering, Northeastern University, Shenyang 110004, PR China.
Journal of colloid and interface science
|February 19, 2025
概括
研究人员开发了一种用于水性离子电池 (ZIB) 的新型混合涂层. 这种涂层有效地防止了阳极上的树生长和副作用反应,提高了电池的性能和寿命.
科学领域:
- 材料科学 材料科学 材料科学
- 电化学 电化学 电化学
- 储能 储能 储能 储能 储能 储能
背景情况:
- 水性离子电池 (ZIBs) 是下一代能源存储的前景.
- 阳极的不稳定性,包括树突的生长和副作用,限制了ZIB的实际应用.
研究的目的:
- 设计和评估ZIB中阳极的新型无机金属混合涂层.
- 通过修改阳极/电解质接口来提高阳极的电化学性能和稳定性.
主要方法:
- 制造具有优化电气双层结构的无机金属混合涂层.
- 在对称和全细胞中涂层阳极的电化学测试.
- 分析离子解溶,核化过度潜力和扩散过程.
主要成果:
- 混合涂层有效地促进了离子溶解,并抑制了不必要的副作用.
- 涂层阳极显著提高了稳定性,抑制了树的生长和腐蚀.
- 对称的电池实现了长周期寿命 (1480小时在1 mA cm−2) 低超电位 (∼34 mV) 和保持性能在更高的电流密度 (1000小时在3 mA cm−2).
结论:
- 混合涂层有效调节阳极/电解质接口,提高ZIB的性能.
- 这种方法为开发稳定和高性能水性离子电池提供了一个可行的策略.
相关概念视频
Extraction: Advanced Methods
402
Metal ions can be separated from one another by complexation with organic ligands–the chelating agent– to form uncharged chelates. Here, the chelating agent must contain hydrophobic groups and behave as a weak acid, losing a proton to bind with the metal. Since most organic ligands used in this process are insoluble or undergo oxidation in the aqueous phase, the chelating agent is initially added to the organic phase and extracted into the aqueous phase. The metal-ligand complex is...
402
EDTA: Auxiliary Complexing Reagents
527
EDTA titrations are usually carried out in highly basic conditions, where the fully deprotonated form of EDTA, Y4−, actively complexes with the free metal ions in the solution. Several metal ions precipitate as hydrous oxide (hydroxides, oxides, or oxyhydroxides) under these conditions, lowering the concentration of free metal ions in the solution. For this reason, auxiliary complexing agents or ligands such as ammonia, tartrate, citrate, or triethanolamine are used in EDTA titrations to...
527
Corrosion of Reinforcement
156
The corrosion of steel reinforcement within concrete is a process influenced by the material's inherent properties and external factors. The high pH level of around 13, provided by calcium hydroxide present in concrete, initially protects the steel reinforcement by promoting the formation of a passive iron oxide layer on its surface.
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
156
Electrodeposition
571
Electrodeposition is a technique used to separate an analyte from interferents by electrochemical processes. Here, the analyte is a metal ion that can be deposited on an electrode immersed in the sample solution. The electrochemical setup consists of an anode and a cathode. When an electric current is applied to the setup, oxidation occurs at the anode. At the cathode, which consists of a large metal surface, metal ions undergo reduction and deposit onto the surface.
Electrodeposition can...
Electrodeposition can...
571
Formation of Complex Ions
23.2K
A type of Lewis acid-base chemistry involves the formation of a complex ion (or a coordination complex) comprising a central atom, typically a transition metal cation, surrounded by ions or molecules called ligands. These ligands can be neutral molecules like H2O or NH3, or ions such as CN− or OH−. Often, the ligands act as Lewis bases, donating a pair of electrons to the central atom. These types of Lewis acid-base reactions are examples of a broad subdiscipline called coordination...
23.2K
Corrosion
23.6K
The degradation of metals due to natural electrochemical processes is known as corrosion. Rust formation on iron, tarnishing of silver, and the blue-green patina that develops on copper are examples of corrosion. Corrosion involves the oxidation of metals. Sometimes it is protective, such as the oxidation of copper or aluminum, wherein a protective layer of metal oxide or its derivatives forms on the surface, protecting the underlying metal from further oxidation. In other cases, corrosion is...
23.6K