快速化的SBS/环氧改性青粘合剂的高温性能的风湿学研究
Lei Feng1, Xinyong Zhang1, Tianyu Sha2
1Taihang Urban and Rural Construction Group Co., Ltd., 569 Shitong Rd., Shijiazhuang 050200, China.
Polymers
|March 13, 2025
概括
一种新型的快速化的环氧树脂 styrene-butadiene-styrene (ER-SBS-T) 修饰剂显著增强了青粘合剂.
科学领域:
- 材料科学 材料科学 材料科学
- 土木工程 土木工程是指土木工程.
- 聚合物化学 聚合物化学
背景情况:
- 青粘合剂的修改对于改善路面性能至关重要.
- 需要新的修饰剂来增强青的高温性能.
- 环氧树脂 styrene-butadiene-styrene (ER-SBS-T) 是一种用于青的新型复合材料修饰剂.
研究的目的:
- 为了研究使用ER-SBS-T.修改的青粘合剂的高温性能.
- 为了评估ER-SBS-T作为快速青改性剂的有效性.
- 为了比较ER-SBS-T改性青与传统的SBS改性青.
主要方法:
- 测试透度,软化点和60°C的运动粘度.
- 执行多重应力爬行恢复 (MSCR) 测试.
- 使用零剪切粘度 (ZSV) 试验和风湿学模型 (交叉模型).
主要成果:
- ER-SBS-T显著提高了青粘合剂的高温性能.
- 经ER-SBS-T改性青的高温性能与SBS改性青相比较.
- 显著改善的最佳ER-SBS-T含量超过6%,分级的参考温度为70°C.
结论:
- ER-SBS-T是一种有效的修饰器,可以提高青粘合剂的高温性能.
- 克罗斯的风湿学模型适用于确定ER-SBS-T修改青中的ZSV.
- 这种修饰剂为耐用青路面提供了一个有前途的解决方案.
相关概念视频
Hot Weather Concreting
52
Concreting at elevated temperatures accelerates the hydration process, leading to quicker setting but potentially reducing the long-term strength of the concrete structure. Additionally, low air humidity fosters rapid moisture loss from the concrete, resulting in reduced workability, pronounced plastic shrinkage, and a higher likelihood of crazing.
Mitigating the heat increase in concrete can be economically achieved by shading aggregate stockpiles to prevent heating from solar radiation,...
Mitigating the heat increase in concrete can be economically achieved by shading aggregate stockpiles to prevent heating from solar radiation,...
52
Design Example: Managing Concrete Workability
67
This example deals with managing the workability of concrete for a raft foundation project under hot weather conditions. Workability is crucial for ensuring the concrete is easy to place, compact, and finish. In this scenario, a slump test — a common method to measure the workability of fresh concrete — initially indicated low workability. This was attributed to the rapid water loss from the concrete mix, exacerbated by the high temperatures causing the course aggregates to heat up.
67