概括
高能离子辐射显著改变聚乙烯.
科学领域:
- 材料科学 材料科学 材料科学
- 聚合物物理 聚合物物理
- 辐射的影响 辐射影响
背景情况:
- 了解聚合物在辐射下的机械特性对于材料设计至关重要.
- 聚乙烯对机械应力的反应受辐射等外部因素的影响.
- 之前的研究表明,不同类型的辐射对聚合物的影响各不相同.
研究的目的:
- 研究离子辐射对聚乙烯机械变形的影响.
- 量化辐射剂量,机械应力和材料特性之间的关系.
- 为了比较离子辐射和电子辐射对聚乙烯的影响.
主要方法:
- 在不同机械应力和辐射剂量下对聚乙烯变形的实验研究.
- 用特定剂量的离子对聚乙烯样品进行辐射 (1.5 × 106到1.0 × 109离子/秒).
- 使用作者开发的框架,对未被辐射和被辐射的聚乙烯的应力-应变曲线进行数值建模.
主要成果:
- 离子辐射 (147 MeV) 显著改变了聚乙烯的变形和强度特性.
- 增加的辐射剂量 (高达109颗/秒) 导致机械应力率增加2.5倍.
- 聚乙烯在辐射后表现出增强的延长和撕裂性能,与失去了可塑性的烯不同.
结论:
- 高能离子辐射提高了聚乙烯在更高的应变值的机械性能.
- 与电子辐射不同的是,147 MeV的离子辐射不会降低聚乙烯的强度.
- 该研究量化了分子链中的变形扭曲,作为辐射流动的函数.
更多相关视频
11:17Synthesis of Programmable Main-chain Liquid-crystalline Elastomers Using a Two-stage Thiol-acrylate Reaction
Published on: January 19, 2016
21.4K
08:31Sample Preparation and Experimental Design for In Situ Multi-Beam Transmission Electron Microscopy Irradiation Experiments
Published on: June 27, 2022
1.6K
相关概念视频
Plastic Behavior
175
A material's elastic behavior is characterized by the disappearance of stress once the load is removed, allowing the material to return to its original state. However, when stress surpasses the yield point, yielding commences, marking the onset of plastic deformation or permanent set. This change from elastic to plastic behavior is influenced by the peak stress value and the duration before the load is removed. An intriguing observation occurs when a specimen is loaded, unloaded, and...
175
Plastic Deformations
76
It is essential to understand how structural members behave under plastic deformation when the bending stress exceeds the material's yield strength. This state of deformation permanently alters the shape of the member, in contrast to the linear elastic behavior observed before yielding. The strain at any point in the member is expressed in terms of maximum strain. Notably, the neutral axis, which coincides with the centroid during elastic bending, shifts away from the centroid under plastic...
76
Polymer Classification: Architecture
2.6K
Polymers are classified as linear or branched on the basis of their chain architecture. The polymer chains in linear polymers have a long chain-like structure with minimal to no branching at all. Even if a polymer features large substituent groups on the monomer, which appear as branches to the skeleton, it is not considered a branched polymer. A branched polymer contains secondary polymer chains that arise from the main polymer chain. The branching occurs when the polymer growth shifts from...
2.6K
Plasticity
2.1K
Plasticity is the property where an object loses its elasticity and undergoes irreversible deformation, even after the deformation forces are eliminated. If a material deforms irreversibly without increasing stress or load, then this is called ideal plasticity. For example, when a force is applied to an aluminum rod, it changes its shape, but it does not return to its original shape once the force is removed. Plastic deformation or ductility is thus a permanent deformation or change in the...
2.1K
Residual Stresses
187
Residual stresses reside in a structure even after removing the original stress inducer. This phenomenon often arises from varied plastic deformations across different parts of a structure. Consider a rod stretched beyond its yield point. It will not regain its original length due to permanent deformation. Even after load removal, the rod does not entirely lose stress because of uneven plastic deformations, resulting in residual stresses. The computation of these stresses in structures is...
187
Plastic Deformations of Members with a Single Plane of Symmetry
84
When a structural member undergoes plastic deformation due to bending, it is crucial to understand the position of the neutral axis and the stress distribution. This member, characterized by a single plane of symmetry, exhibits a uniform stress distribution, with negative stress above the neutral axis and positive stress below. Notably, the neutral axis does not align with the centroid of the cross-section. This misalignment is typical in cases where the cross-section is not rectangular or...
84