用增量和雪技术进行的1类复合材料修复的断裂阻力值的比较
Rahime Zeynep Erdem1, Ayşenur Kuşuçar2, Semanur Özüdoğru3
1Department of Restorative Dentistry, Faculty of Dentistry, Afyonkarahisar Health Sciences University, Afyonkarahisar, Turkey, zeynepguvendi@hotmail.com.
American journal of dentistry
|May 5, 2025
概括
雪技术用于放置短纤维增强复合材料 (SFRC) 降低了牙骨折阻力. 传统的增量技术 (IT) 保持了高的机械性能,类似于对照组.
科学领域:
- 牙科材料科学 牙科材料科学
- 生物材料工程 生物材料工程
- 恢复性牙科 恢复性牙科
背景情况:
- 牙科复合材料对于牙修复至关重要.
- 了解放置技术会影响修复的寿命.
- 短纤维增强复合材料 (SFRC) 提供潜在的好处.
研究的目的:
- 用增量技术 (IT) 与雪技术 (SP) 来比较用SFRC恢复的牙的骨折抵抗.
- 评估不同复合材料放置方法对牙机械完整性的影响.
主要方法:
- 用SFRC与IT或SP技术进行了修复.
- 牙经历了热循环,以模拟口腔内条件.
- 使用机械测试机器测量断裂阻力.
- 使用ANOVA和Tukey HSD测试进行了统计分析.
主要成果:
- 两组之间观察到骨折抵抗的显著差异.
- 雪技术 (SFRC-SP) 与增量技术 (SFRC-IT) 和正控相比显示出明显较低的断裂阻力.
- 增量技术 (SFRC-IT) 证明了与对照组相比的骨折阻力.
结论:
- 雪技术损害了SFRC修复的机械强度.
- 增量技术保留了SFRC的机械特性,实现了与控制器相似的结果.
- 在SFRC的临床应用中,应考虑增量技术,以获得最佳的骨折阻力.
更多相关视频
相关概念视频
Abrasion Resistance of Concrete
80
Abrasion resistance is an essential characteristic of concrete that determines its durability and longevity under various wear conditions. Concrete surfaces are vulnerable to different types of abrasion. For instance, surfaces may wear down due to the constant movement of vehicles or be eroded by solids carried in water, as seen in concrete canal linings. Specific tests are conducted to measure the abrasion resistance of concrete.
One such test is the revolving disc test, where three plates...
One such test is the revolving disc test, where three plates...
80
Frost Resistant Concrete
62
Concrete's susceptibility to frost damage during freeze-thaw cycles demands strategic measures to enhance its frost resistance. Employing techniques like air entrainment, adjusting the water-cement ratio, proper curing, and selecting appropriate aggregates are essential.
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of...
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of...
62
Non-destructive Tests for Concrete Strength
98
The rebound hammer test, also known as the Schmidt hammer test, is a non-destructive technique for evaluating the hardness of concrete and, indirectly, the strength of concrete. It operates on the principle that the rebound of a spring-driven mass from a concrete surface correlates to the surface's hardness. The device comprises a mass within a tubular housing, a spring mechanism, and a plunger that strikes the concrete. Upon release, the energy imparted to the mass by the spring causes it...
98