Sahar M N Bukhary1, Hisham I Othman2,3, Ghada Mansour2,4

  • 1Department of Oral Biology, Faculty of Dentistry, King Abdulaziz University, Jeddah, Saudi Arabia.

概括

严重的牙周炎会显著改变牙根的质,导致不规则的表面和元素组成的变化. 这可能会使牙疾病恶化,并影响牙周整体健康.