重新连接还是恢复? 不复杂的皇冠骨折的骨折阻力使用各种中间材料
Soner Sismanoglu1, Vasfiye Isik2
1Department of Restorative Dentistry, Faculty of Dentistry, Istanbul University-Cerrahpaşa, Istanbul, Turkey.
概括
对于不复杂的皇冠骨折,预热复合材料和自粘树脂水泥与直接复合材料树脂相比,提供优越的断裂阻力. 这一发现有助于选择最佳的粘合材料,用于牙碎片的重新连接.
科学领域:
- 牙科 牙科是指牙科的专业.
- 牙科材料科学 牙科材料科学
背景情况:
- 不复杂的皇冠骨折是常见的牙损伤.
- 碎片重新连接是一种保守的治疗选择.
- 重复连接碎片的机械稳定性取决于所使用的粘合材料.
研究的目的:
- 为了比较不同粘合材料的断裂阻力,以便重新连接碎片.
- 评估预热复合材料和自粘树脂水泥与直接复合材料树脂.
主要方法:
- 60个人类大切口器被 subjected to模拟的皇冠骨折. 在这个研究中,60个人类大切口器经历了模拟的皇冠骨折.
- 牙被分为五组:控制,直接复合,可流动复合,预热复合和自粘树脂水泥.
- 在使用通用测试机器进行热循环后,对断裂阻力进行了评估.
主要成果:
- 对照组表现出最高的断裂阻力,而直接复合树脂表现出最低的.
- 预热复合材料和自粘树脂水泥表现出比直接复合材料树脂明显更高的抗破性.
- 在可流动复合材料,预热复合材料和自粘树脂水泥中没有观察到裂痕阻力显著差异.
结论:
- 预热复合材料和自粘树脂水泥在不复杂的皇冠骨折中增强碎片重新连接的断裂抵抗力.
- 材料的选择对于改善牙碎片复合手术的长期临床成功至关重要.
相关概念视频
Fractures: Bone Repair
3.7K
Treatment for a fracture is based on the type of break, the bone affected, and the patient's age.
Minor fractures with no bone displacement are treated by immobilizing the fractured bone using a cast or splint. However, in the case of fractures with displaced bones, the broken bones are repositioned before immobilization to ensure successful healing without deformation and loss of function. The realignment of fractured bone ends is performed through a process called reduction. If the...
Minor fractures with no bone displacement are treated by immobilizing the fractured bone using a cast or splint. However, in the case of fractures with displaced bones, the broken bones are repositioned before immobilization to ensure successful healing without deformation and loss of function. The realignment of fractured bone ends is performed through a process called reduction. If the...
3.7K
Stress-Strain Diagram - Brittle Materials
2.8K
Brittle materials, including glass, cast iron, and stone, exhibit unique characteristics. They fracture without considerable change in their elongation rate, indicating that their breaking and ultimate strength are equivalent. Such materials also show lower strain levels at the point of rupture. The failure in brittle materials predominantly results from normal stresses, as evidenced by the rupture created along a surface perpendicular to the applied load. These materials do not display...
2.8K