涂层标记砂的制备和性能评估,用于水平井的细分断裂
Cheng Jing1,2, Pengye Zhao1,2, Gang Zheng3
1School of Petroleum Engineering, Xi'an Shiyou University, Xi'an, Shaanxi 710065, China.
ACS omega
|August 18, 2025
概括
涂层的标志性沙子可以实时监测横向井中的断裂效应和流体产量. 这项技术优化了压裂程序,以从非传统资源中提升石油和天然气的回收.
科学领域:
- 石油工程是石油工程中的一个.
- 材料科学 材料科学 材料科学
背景情况:
- 多阶段破裂对于开发非传统石油和天然气资源至关重要.
- 在水平井中监测压裂效率和产量概况对于优化至关重要.
研究的目的:
- 研究一种用于缓释涂层标记砂的制备方法.
- 优化推进剂,涂层和有效的标记元件,以提高性能.
主要方法:
- 开发了一种用于缓释涂层标记砂的制备方法.
- 评估的性能参数包括颗粒大小,盐度,温度,pH值和泥速度.
- 评估环境因素对追踪剂释放率的影响.
主要成果:
- 颗粒大小和盐度对完整涂层的缓释性能影响最小.
- 酸性条件增强痕迹剂的释放,而性条件抑制它.
- 较高的温度增加了追踪器释放率,遵循设定的速度规律,直到达到临界速度.
结论:
- 涂层缓释标记砂为实时监测水平井断裂提供了一种可行的方法.
- 优化的追踪器准备为提高水平井开发效率提供了理论基础.
- 了解环境对追踪剂释放的影响是有效应用的关键.
相关概念视频
Design Example: Aggregate Gradation
147
The right type and quality of aggregates are crucial for concrete as they significantly influence its properties, mix proportions, and cost-effectiveness. If different sources are available for sand, the commonly used fine aggregate in concrete, the selection of sand is primarily based on its gradation.
The grading, or particle-size distribution, of sand is determined using sieve analysis, with standard sizes ranging from 150 μm to 10 mm (ASTM No. 100 sieve to 3⁄8 in. sieve). Sand is...
The grading, or particle-size distribution, of sand is determined using sieve analysis, with standard sizes ranging from 150 μm to 10 mm (ASTM No. 100 sieve to 3⁄8 in. sieve). Sand is...
147
Shotcrete
148
Shotcrete is a specialized technique where mortar or small aggregate concrete rich in cement content is sprayed onto a surface at high velocity. The force of impact compacts the material and enables it to cling to vertical or overhead areas without sagging. The technique involves layering the shotcrete in stages until it reaches approximately 4 inches in thickness. Operator skill in nozzle management is pivotal in deciding the quality of the shotcrete. Shotcrete is used in constructing tunnel...
148
Segregation in Fresh Concrete
234
Segregation in fresh concrete is a phenomenon where the components of the concrete mix separate, leading to uneven distribution and compromised structural integrity. This separation typically occurs when concrete is subjected to excessive horizontal movement within forms, or when it is dropped from considerable heights or forced through narrow, winding paths. As a result, heavier coarse aggregate particles settle at the bottom, while lighter, finer materials such as cement and water rise to the...
234
Preplaced Aggregate Concrete
137
Preplaced aggregate concrete is ideal for construction environments that are not easily accessible. The process begins by properly wetting the gap-graded coarse aggregates to remove the dirt, then placing it in the form and compacting it. Voids are filled with a mortar mix pumped under pressure through slotted pipes. This mortar typically consists of Portland cement, pozzolan, fine aggregates, water, and a fluidizing aid. The pozzolan helps reduce bleeding and segregation while improving the...
137
Abrasion Resistance of Concrete
201
Abrasion resistance is an essential characteristic of concrete that determines its durability and longevity under various wear conditions. Concrete surfaces are vulnerable to different types of abrasion. For instance, surfaces may wear down due to the constant movement of vehicles or be eroded by solids carried in water, as seen in concrete canal linings. Specific tests are conducted to measure the abrasion resistance of concrete.
One such test is the revolving disc test, where three plates...
One such test is the revolving disc test, where three plates...
201
Porosity and Absorption of Aggregate
398
Aggregates contain pores of varying sizes; while some are completely enclosed within the particles, others open onto the surface, allowing water to penetrate. The porosity of aggregates is a major factor contributing to the overall porosity of concrete, given that aggregates constitute about three-quarters of concrete's volume.
When all pores in an aggregate are filled with water, the aggregate is considered saturated and surface-dry. If left in dry air, water will evaporate until the...
When all pores in an aggregate are filled with water, the aggregate is considered saturated and surface-dry. If left in dry air, water will evaporate until the...
398