石膏混凝土振动压缩技术参数的设计
Leonid Dvorkin1, Vadim Zhitkovsky1, Yuri Ribakov2
1Department of Building Elements Technology and Materials Science, National University of Water and Environmental Engineering, 33028 Rivne, Ukraine.
Materials (Basel, Switzerland)
|August 28, 2025
概括
本研究介绍了一种使用超硬混合物的振动压缩来生产高强度石膏混凝土的方法. 开发的方法优化了聚合物与石膏的比率和水与石膏的比率,以达到所需的压力强度.
科学领域:
- 材料科学
- 土木工程
- 建筑材料
背景情况:
- 石膏混凝土作为建筑材料具有潜力.
- 开发高性能石膏混凝土的高效生产方法至关重要.
研究的目的:
- 通过振动压缩超硬混合物制造石膏混凝土的方法.
- 建立一种设计这种混凝土组成的方法.
- 模拟技术因素对石膏混凝土性能的影响.
主要方法:
- 使用数学实验设计进行组合分析.
- 获得了强度和密度的实验和统计多项式模型.
- 研究了水分含量,聚合物和振动压缩参数的影响.
主要成果:
- 开发了与石膏混凝土强度和密度相关的技术模型.
- 建立了一个设计振动压混凝土组合的方法.
- 在硬化1天后,达到15至44MPa的压力强度.
结论:
- 建议的方法可以设计具有可预测强度的振动压混凝土.
- 该方法考虑了材料质量,聚合物特性和振动压缩参数.
- 优化的水比率确保了最大的紧缩和所需的性能.
相关概念视频
Vibrating Concrete
185
Mechanical vibrators are instrumental in compacting newly poured concrete within formwork and around reinforcements. This process is essential to eliminate trapped air pockets and establish a dense concrete mass. One widely used method is vibrating by internal vibrators, often referred to as a poker vibrator or immersion vibrator. It is rapidly inserted through the full depth of the freshly laid concrete and slightly extends into the layer below it (which remains in a plastic state). Consistent...
185
Behavior of Concrete Under Compressive Load
268
Concrete exhibits specific behaviors under different compressive loads. Understanding this is crucial for understanding its structural integrity. When concrete undergoes uniaxial compression, it tends to develop cracks that run parallel to the direction of the force. These parallel cracks stem from localized tensile stresses that occur perpendicular to the compression direction. Additionally, angled cracks may appear due to the formation of shear planes.
As the concrete specimen fractures under...
As the concrete specimen fractures under...
268
Dynamic Modulus of Elasticity of Concrete
539
The dynamic modulus of elasticity assesses how a concrete structure deforms under impact or dynamic loads. It is typically higher than the static modulus of elasticity, measured under slow, steady loading conditions.
The sonic test is a common method to determine the dynamic modulus. In this test, a concrete beam, sized either 6 x 6 x 30 inches or 4 x 4 x 20 inches, is clamped at its center. Vibrations are initiated at one end of the beam by an electromagnetic exciter unit powered by...
The sonic test is a common method to determine the dynamic modulus. In this test, a concrete beam, sized either 6 x 6 x 30 inches or 4 x 4 x 20 inches, is clamped at its center. Vibrations are initiated at one end of the beam by an electromagnetic exciter unit powered by...
539
Effects of Air-entrainment in Concrete
140
Air entrainment in concrete significantly enhances the material's durability, especially in environments subjected to freeze-thaw cycles. Introducing small air bubbles into the concrete mix acts as internal voids that accommodate the expansion of water when it freezes, thereby alleviating internal stress and preventing structural cracks. This function is crucial in climates with significant freezing and thawing, as it protects the concrete from repeated stresses that could lead to premature...
140
Manufacture of Concrete Masonry Units
172
The process of manufacturing concrete masonry units begins by mixing stiff concrete composed of Portland cement, aggregates, and water. This mixture is then poured into metal molds. To ensure the concrete settles uniformly and to avoid separation of its components, the mixture in the molds is subjected to vibration. Shortly after, the still-wet blocks are removed from the molds and placed on racks.
These wet blocks are then transported for curing, which can occur in one of two environments: a...
These wet blocks are then transported for curing, which can occur in one of two environments: a...
172
Design Example: Managing Concrete Workability
121
This example deals with managing the workability of concrete for a raft foundation project under hot weather conditions. Workability is crucial for ensuring the concrete is easy to place, compact, and finish. In this scenario, a slump test — a common method to measure the workability of fresh concrete — initially indicated low workability. This was attributed to the rapid water loss from the concrete mix, exacerbated by the high temperatures causing the course aggregates to heat up.
121