对EOR的聚合物-表面活性剂二进制洪水的协同优化:配方,污泥设计和盐度效应的核心规模实验分析
Wenjie Tang1, Patiguli Maimaiti1, Hongzhi Shao1
1Research Institute of Exploration and Development, Xinjiang Oilfield Company, PetroChina, Karamay 834000, China.
Polymers
|August 28, 2025
概括
用0.5%的表面活性剂和0.15%的聚合物混合物优化油的回收率提高了42.19%. 这种化学增强石油回收 (EOR) 方法平衡粘度,界面张力降低和现场应用的操作因素.
科学领域:
- 石油工程
- 化学工程
- 增强石油回收 (EOR)
背景情况:
- 在油田开发的中后阶段, 常规的水淹没效果较差.
- 降低回收率需要使用化学增强石油回收 (EOR) 等先进技术.
- 聚合物-表面活性剂二元浸是改善石油开采的关键EOR技术.
研究的目的:
- 在核心泛滥实验中研究聚合物-表面活性剂二元配方的协同效应.
- 确定最佳度,注入量和盐度条件以提高油的回收.
- 为优化聚合物表面活性剂泛滥的现场应用提供实验数据.
主要方法:
- 使用各种聚合物表面活性剂度和注射量进行了核心泛滥实验.
- 测量表面张力 (IFT),以评估表面活性剂的有效性.
- 通过改变总溶解固体 (TDS) 来分析盐度敏感性,以评估粘度和恢复影响.
主要成果:
- 最佳配方 (0.5%表面活性剂,0.15%聚合物) 的最大增量油回收率为42.19%.
- 这种配方降低了界面张力 (IFT) 到0.007 mN/ m.
- 使用0. 5孔体积 (PV) 的注射体积和具有度梯度的顺序注射体积是最有效的.
- 较高的TDS降低了粘度,而低的TDS提供了最小的恢复增强,尽管粘度更高.
结论:
- 这项研究提供了优化聚合物表面活性剂泛滥策略的实验验证.
- 控制粘度,减少IFT和运行可行性的平衡对于现场成功至关重要.
- 这些发现为使用化学EOR增强成熟油田的石油回收提供了实用见解.
相关概念视频
Colloids
17.9K
Children at play often make suspensions such as mixtures of mud and water, flour and water, or a suspension of solid pigments in water known as tempera paint. These suspensions are heterogeneous mixtures composed of relatively large particles that are visible to the naked eye or can be seen with a magnifying glass. They are cloudy, and the suspended particles settle out after mixing. On the other hand, a solution is a homogeneous mixture in which no settling occurs and in which the dissolved...
17.9K
Factors Affecting Dissolution: Particle Size and Effective Surface Area
1.0K
Dissolution kinetics, an essential aspect of oral drug delivery, is significantly influenced by the drug's particle size. According to the Noyes-Whitney dissolution model, the dissolution rate correlates directly with the drug's surface area. The larger the surface area, the higher the drug's solubility in water, leading to a faster drug dissolution rate. Reducing particle size increases the effective surface area, enhancing the dissolution process. Micronization and nanosizing are...
1.0K