概括
聚合后的时间和固化装置类型不会影响表面粗度,但会增加3D打印永久树脂的微硬度和颜色变化. 这些因素影响了牙科修复的机械和光学特性.
科学领域:
- 材料科学
- 生物材料工程
- 牙科材料
背景情况:
- 3D打印越来越多地用于永久性牙科修复.
- 优化3D打印树脂的特性对于临床成功至关重要.
- 聚合后的过程对材料的特性有很大影响.
研究的目的:
- 评估聚合后时间和固化装置类型对3D打印永久树脂性能的影响.
- 评估经过老化后表面粗度,微硬度和颜色的变化
主要方法:
- 使用50μm层厚的SLA和DLP技术打印样品.
- 使用蓝色LED和紫外线LED装置进行后聚合,持续时间不同 (10-60分钟).
- 表面粗度,微硬度和颜色在最初和5000个老化周期后被测量,并通过双向ANOVA分析.
主要成果:
- 聚合后的时间和固化装置类型没有显著影响表面粗度.
- 用SLA打印的样本显示,随着更长的UV LED后聚合,微硬度增加.
- 随着两种打印机类型的延长后聚合时间,颜色变化和白度指数增加.
结论:
- 聚合后的参数影响3D打印永久树脂的微硬度和光学特性.
- 表面粗度不受这些参数的影响.
- 优化后聚合对于实现牙科修复所需的机械和美学效果至关重要.
相关概念视频
Curing Methods
121
Concrete members with a small surface-to-volume ratio are cured by oiling and moistening the forms before casting the concrete member. These forms can be left in place for a prolonged period to prevent moisture loss, and can be wetted if made of a material suitable for wetting. If the forms are removed early, the concrete member is moistened and covered with polythene sheets to maintain moisture. For large horizontal concrete surfaces exposed to dry weather, a temporary covering is suspended...
121
Accelerated Curing of Concrete
256
Accelerating concrete curing is achieved by applying heat and additional moisture. This process accelerates the hydration of the cement, resulting in an earlier strength gain in the concrete. Steam curing is a method wherein the concrete products are either transported through a chamber on a conveyor belt or encased in plastic, allowing steam at atmospheric pressure to circulate freely around them. This process begins with a phase of moist curing that typically lasts between 3 to 5 hours, after...
256
Curing of Concrete
166
The hydration of cement takes place within the water-filled capillary pores. However, environmental elements can disrupt this process by evaporating water from the concrete surfaces. Sealed concrete with a water-cement ratio below 0.5 experiences self-desiccation, leading to water loss. The water loss in concrete is mitigated by curing. This technique involves keeping the concrete saturated to maintain the necessary temperature and moisture conditions, to optimally fill the spaces in the cement...
166