在 WAAM NAB 的重叠与基板区域中的微观结构和化侵蚀行为
Xiang Cai1, Shuo Wang2, Dun Miao3
1School of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212003, China.
Ultrasonics sonochemistry
|September 13, 2025
概括
-铜 (NAB) 合金的电弧增材制造显示了微观结构差异,影响了洞穴侵蚀 (CE). 重叠区域提供了更好的CE电阻,尽管腐蚀显著加快了材料损失.
科学领域:
- 材料科学 材料科学 材料科学
- 添加剂制造 添加剂制造 添加剂制造
- 腐蚀科学 腐蚀科学
背景情况:
- 铜 (NAB) 对于海洋应用至关重要.
- 电弧增材制造 (WAAM) 提供了独特的微观结构可能性.
- 了解化侵蚀 (CE) 和腐蚀协同作用对于材料耐用性至关重要.
研究的目的:
- 研究WAAM处理的NAB微结构对CE的影响.
- 分析CE和腐蚀的协同影响.
- 确定材料降解中的主要机制.
主要方法:
- 微观结构特征 (颗粒大小,相位含量,沉物).
- 在合成海水中进行洞穴侵蚀测试.
- 对协同作用的CE-腐蚀效应的分析.
主要成果:
- 叠加的区域具有更细的粒度,更高的β'阶段,和不同于基板的沉物.
- 在CE期间,重叠区域的累积质量损失较小,但初始速度较快.
- 一个经CE后形成的工作硬化层,表面附近的峰值硬度.
- 腐蚀-CE协同作用对质量损失贡献了52%,腐蚀促进了CE.
结论:
- 来自WAAM的NAB微结构显著影响CE电阻.
- 腐蚀和CE的协同效应是相当大的,腐蚀加剧了CE.
- 材料降解是机械和电化学过程之间的复杂相互作用.
更多相关视频
12:26Fabrication, Operation and Flow Visualization in Surface-acoustic-wave-driven Acoustic-counterflow Microfluidics
Published on: August 27, 2013
17.7K
07:23Fabrication of Nanoheight Channels Incorporating Surface Acoustic Wave Actuation via Lithium Niobate for Acoustic Nanofluidics
Published on: February 5, 2020
6.2K
相关概念视频
Van der Waals Interactions
58.1K
Atoms and molecules interact with each other through intermolecular forces. These electrostatic forces arise from attractive or repulsive interactions between particles with permanent, partial, or temporary charges. The intermolecular forces between neutral atoms and molecules are ion–dipole, dipole–dipole, and dispersion forces, collectively known as van der Waals forces.
58.1K
Long-patch Base Excision Repair
6.3K
Since the discovery of the two BER pathways, there has been a debate about how a cell chooses one pathway over the other and the factors determining this selection. Numerous in vitro experiments have pointed out multiple determinants for the sub-pathway selection. These are:
6.3K
Deleterious Substances in Aggregate
867
Deleterious substances in aggregates can be detrimental to the quality and durability of concrete. These substances include organic impurities like loam, which interfere with cement hydration and are usually present in the sand. These prevent a good bond between aggregate and cement paste. Organic impurities can be detected using the colorimetric test, where the darkness of a solution after agitation indicates the level of organic content.
Another type of impurity is clay and fine material that...
Another type of impurity is clay and fine material that...
867
Microcracking in Concrete
614
Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
614