电池中的金属阳极的电腐蚀
Chen-Xi Bi1,2, Yu-Jie Zhu1,2, Xi-Yao Li3
1School of Materials Science and Engineering, Beijing Institute of Technology, Beijing 100081, P. R. China.
Journal of the American Chemical Society
|September 16, 2025
概括
聚硫化物对硫电池中的金属阳极造成电腐蚀. 预先构建一个保护层可以显著增加57%的电池寿命.
科学领域:
- 电化学
- 材料科学
- 能量储存
背景情况:
- -硫 (Li-S) 电池在理论上具有很高的能量密度,但周期寿命很短.
- 主要的限制是由于聚硫化物 (LiPS) 腐蚀而导致的金属阳极的不稳定性.
研究的目的:
- 确定电池中极降解背后的机制.
- 制定一种策略,以减轻LiPS腐蚀并提高Li-S电池的循环稳定性.
主要方法:
- 研究了LiPS对Li金属阳极产生的电腐蚀.
- 分析了LiPS腐蚀动力学对电极电位和Li沉积的影响.
- 设计了一种富含化的固体电解质交相 (SEI) 来使金属阳极无源化.
主要成果:
- 由于空间异质的LiPS腐蚀导致非均的Li沉积和加速的细胞衰竭.
- 预制的富含化物SEI有效地使金属阳极无能化.
- 经过修改的-S电池在恶劣条件下增加了57%的循环寿命.
结论:
- 电腐蚀是导致Li-S电池不均沉积和故障的关键机制.
- 通过保护性SEI层使Li金属阳极受体化对于实现长周期Li-S电池至关重要.
- 开发的被动化战略为推进Li-S电池技术提供了一个有前途的途径.
更多相关视频
相关概念视频
Voltaic/Galvanic Cells
63.0K
Spontaneous Chemical Reactions
Spontaneous redox reactions occur abundantly in nature. The chemical reaction occurring in a disposable AA battery powering our remote controls is one such example of a spontaneous redox reaction. Another example is the immersion of coiled copper wire into an aqueous silver nitrate solution. The reaction shows a gradual, visually impressive color change from colorless to bright blue and the formation of a grey precipitate on the copper wire. In this experiment,...
Spontaneous redox reactions occur abundantly in nature. The chemical reaction occurring in a disposable AA battery powering our remote controls is one such example of a spontaneous redox reaction. Another example is the immersion of coiled copper wire into an aqueous silver nitrate solution. The reaction shows a gradual, visually impressive color change from colorless to bright blue and the formation of a grey precipitate on the copper wire. In this experiment,...
63.0K
Batteries and Fuel Cells
30.7K
A battery is a galvanic cell that is used as a source of electrical power for specific applications. Modern batteries exist in a multitude of forms to accommodate various applications, from tiny button batteries such as those that power wristwatches to the very large batteries used to supply backup energy to municipal power grids. Some batteries are designed for single-use applications and cannot be recharged (primary cells), while others are based on conveniently reversible cell reactions that...
30.7K
Electrolysis
30.2K
In a galvanic cell, the electrical work is done by a redox system on its surroundings as electrons produced by the spontaneous redox reactions are transferred through an external circuit. Alternatively, an external circuit does work on a redox system by imposing a voltage sufficient to drive an otherwise nonspontaneous reaction in a process known as electrolysis. For instance, recharging a battery involves the use of an external power source to drive the spontaneous (discharge) cell reaction in...
30.2K
Electrogravimetric Analysis: Overview
744
Electrogravimetric analysis measures the weight of an analyte deposited electrolytically onto a suitable working electrode. This method involves applying a potential to a pre-weighed electrode submerged in a solution, which results in the desired substance being deposited through reduction at the cathode or oxidation at the anode. The electrode's weight is recorded after deposition, and the difference in weight gives the analyte's weight in the solution.
To test the completeness of the...
To test the completeness of the...
744
Formation of Complex Ions
25.7K
A type of Lewis acid-base chemistry involves the formation of a complex ion (or a coordination complex) comprising a central atom, typically a transition metal cation, surrounded by ions or molecules called ligands. These ligands can be neutral molecules like H2O or NH3, or ions such as CN− or OH−. Often, the ligands act as Lewis bases, donating a pair of electrons to the central atom. These types of Lewis acid-base reactions are examples of a broad subdiscipline called coordination...
25.7K
Standard Electrode Potentials
49.9K
On comparing the reactivity of silver and lead, it is observed that the two ionic species, Ag+ (aq) and Pb2+ (aq), show a difference in their redox reactivity towards copper: the silver ion undergoes spontaneous reduction, while the lead ion does not. This relative redox activity can be easily quantified in electrochemical cells by a property called cell potential. This property is commonly known as cell voltage in electrochemistry, and it is a measure of the energy which accompanies the charge...
49.9K