光热用于现场处理高盐度废水的零液体排放
Xuxiao Luo1, Yingru Li1, Xin Yang1
1State Environmental Protection Key Laboratory of Synergetic Control and Joint Remediation for Soil & Water Pollution, College of Ecology and Environment, Chengdu University of Technology, Chengdu, 610059, China; Institute of Industrial Technology, Chengdu University of Technology, Yibin, Sichuan, China.
Environmental research
|November 7, 2025
概括
我们从铁尾矿开发了一种耐用的光热,用于高盐度废水的可持续零液体排放 (ZLD). 这种坚固的材料可实现高效的太阳能驱动蒸发,为工业处理提供了具有成本效益和可扩展的解决方案.
科学领域:
- 环境工程 环境工程
- 材料科学 材料科学 材料科学
- 可持续技术 可持续技术
背景情况:
- 高盐度的废水面临着重大处理挑战.
- 现有的光热零液体排放 (ZLD) 技术面临成本和材料耐用性的限制.
- 开发强大且可扩展的解决方案对于有效的废水管理至关重要.
研究的目的:
- 为太阳能驱动的废水处理设计一种机械强,耐用的光热材料.
- 评估用于高盐度废水的开发材料的性能和可扩展性.
- 为光热ZLD建立一个工业上可行的途径.
主要方法:
- 使用压缩铁尾部制造光热 (P-B).
- 机械测试 (压力强度) 和老化模拟以评估耐用性.
- 实验室和现场验证P-B用于太阳能驱动的高盐度废水界面蒸发.
主要成果:
- 在P-B表现出高压力强度 (26.9MPa),并在一年的模拟老化后保持了>90%的强度.
- 在实验室测试中,在模拟的阳光下,蒸发率达到1.65kg m−2·h−1.
- 现场验证证明了可扩展性,在自然阳光下处理2000公斤废水,峰值速度为6.25公斤m−2·h−1.
结论:
- 开发的光热为太阳能发电的ZLD提供了一种机械强和耐用的解决方案.
- 该P-B技术是可扩展和有效的高度工业废水的现场处理.
- 这项工作弥合了光热创新和实际的大规模废水处理应用之间的差距.
相关概念视频
Bricks
391
Bricks, a fundamental building material, are crafted from fired clay and exhibit a range of shapes, sizes, and colors. The production process starts with extracting local clay or shale, which is then crushed, ground, and screened for a fine texture. The refined material is blended with water, creating a pliable mixture that can be formed into bricks using one of three processes: soft mud, dry press, or stiff mud methods.
Soft mud bricks are shaped in molds with high moisture content and can be...
Soft mud bricks are shaped in molds with high moisture content and can be...
391
Masonry in Cold and Hot Weather Conditions
324
In cold weather, masonry construction requires specific precautions to ensure mortar does not freeze before curing, as this can significantly weaken its strength and watertightness. Mortar temperature should be maintained between 60°F and 80°F to support proper hydration and curing. Below 40°F, mortar water must be heated, but should not exceed 120°F as high temperatures can reduce mortar's compressive and bond strength.
Other key practices include keeping masonry units...
Other key practices include keeping masonry units...
324