概括
拜耳红泥 (BRM) 可以在不损失强度的情况下取代水泥高达5%. 较高的数量会降低强度,但BRM可以安全地用作补充的水泥材料,有助于废物管理.
科学领域:
- 材料科学 材料科学 材料科学
- 土木工程 土木工程是指土木工程.
- 环境科学 环境科学
背景情况:
- 拜耳红泥 (BRM) 是炼的主要工业副产品.
- 可持续利用BRM对于行业的废物管理至关重要.
研究的目的:
- 评估来自山东新发集团的拜耳红泥 (BRM) 作为部分水泥替代品.
- 评估BRM对水泥性质和微观结构发展的影响.
- 为了确定BRM混合砂的环境安全性.
主要方法:
- 用0.5%,1%,5%,10%和15%的重量用BRM替代水泥.
- 在3天和28天评估定位时间和压力强度.
- 使用XRD,TG/DTG和SEM进行微结构分析.
- 通过毒性特征漏程序 (TCLP) 进行漏性测试.
主要成果:
- 在可接受的范围内,BRM的加入稍微延长了设置时间.
- 压力强度与对照值相比,最高可达到5%的BRM替代.
- 较高的BRM含量 (10%,15%) 显著降低了压力强度.
- 微结构分析表明BRM充当了微填充物和核化部位.
- TCLP的结果证实重金属度低于监管值.
结论:
- 新发集团的BRM可以有效地用作补充的水泥材料,最多可取代10%.
- 低于10%的BRM纳入显示了可持续固体废物管理的潜力.
- 由于重金属漏能力低,BRM混合砂对环境造成的风险最小.
相关概念视频
Pozzolans
458
Pozzolans are siliceous or aluminous materials blended with Portland cement. They interact with the calcium hydroxide produced during the hydration of Portland cement and contribute to improved strength and durability of concrete. The pozzolanic activity, a measure of a pozzolan's effectiveness, is typically assessed using the strength activity index, as defined in ASTM C 618-93, which calculates the ratio of the compressive strength of cement mixtures with and without pozzolan.
Fly ash is...
Fly ash is...
458
Additives and Fillers in Concrete
314
Additives and fillers are integral to enhancing the properties of concrete. Pozzolans and blast-furnace slag are additives or admixtures due to their reactions with calcium hydroxide released during cement hydration. Fillers, which are finely ground and similar in fineness to Portland cement, improve concrete attributes such as workability density, and reduce capillary bleeding or cracking. Some fillers possess hydraulic properties or participate in benign reactions within the cement paste.
The...
The...
314
Types of Cement II
377
Portland blast-furnace cement is made by blending Portland cement clinker with granulated blast-furnace slag, which accounts for 25 to 65 percent of the cement's weight. Despite its similarities to ordinary Portland (Type I) cement in terms of fineness and setting times, its early strength is lower, though it achieves comparable strength later on. It's particularly suited for mass concrete structures and marine environments due to its lower heat of hydration and superior sulfate...
377
Hydration of Cement
770
Hydration of cement is a chemical reaction between cement particles and water. This process occurs primarily through two mechanisms: through-solution and topochemical. In the through-solution process, anhydrous compounds dissolve into their constituents, hydrates form in the solution, and then precipitate from the supersaturated solution. The topochemical process involves solid-state reactions at the cement particle surface. The through-solution process dominates the topochemical process at the...
770
Aggregate Cement Ratio
517
The Aggregate Cement ratio refers to the weight of aggregate divided by the weight of cement in a concrete mix. Altering this ratio has profound effects on the concrete's properties. This ratio plays a pivotal role in determining the strength, workability, and durability of concrete. When the Aggregate Cement ratio is higher, the mix is leaner, meaning it has less cement paste to lubricate the aggregate, potentially making the concrete less workable. Such mixes, known as lean, enhance the...
517
Superplasticizers
281
Superplasticizers are advanced admixtures that enhance the workability of concrete by lowering the water content without compromising the strength of the material. These substances are highly effective water reducers, improving concrete flow, making it easier to work with, and enabling concrete to reach inaccessible areas or densely reinforced sections without mechanical vibration. The key components in superplasticizers are either sulfonated melamine or naphthalene formaldehyde condensates,...
281