赞坦 (XG) 和碳素甲基纤维素 (CMC-Na) 通过增加粘度来提高消防泡的稳定性. 聚烯胺 (PAM) 在低度提供好处,但在更高水平上阻碍了泡性能.
科学领域:
- 材料科学 材料科学 材料科学
- 化学工程是化学工程的重要组成部分.
- 消防安全工程 消防安全工程
背景情况:
- 聚合物稳定剂对于提高消防泡的稳定性和性能至关重要.
- 短链碳表面活性剂越来越多地用于消防泡配方.
研究的目的:
- 为了评估香甘 (XG),聚烯胺 (PAM) 和糖甲基纤维素 (CMC-Na) 对灭火泡溶液的影响.
- 研究这些稳定剂对界面特性,表面粘度和泡性能的影响.
主要方法:
- 介面张力分析 介面张力分析
- 粘度测量 粘度测量 粘度测量
- 动态泡分析的动态泡分析
- 泡排水测试 泡排水测试
主要成果:
- XG和CMC-Na略有降低了界面活性,但显著增加了表面粘度,改善了泡的稳定性并减少了排水.
- PAM显示了双重效应:在度低于0.06%的度下增强泡稳定性,但损害泡形成,并且由于界面聚合和网络形成,在更高度下增加排水.
- 0.10重量%的XG导致粗化时间为724.64秒,25%的排水时间为1519.15秒.
结论:
- 赞坦和CMC-Na是基于短链碳表面活性剂的灭火泡的有效聚合物稳定剂,主要是通过增加粘度.
- 聚烯胺的有效性取决于度,需要仔细优化以避免对泡性能产生负面影响.
- 这些发现为在先进的消防泡系统中应用聚合物稳定剂提供了关键的见解.
相关概念视频
Anionic Chain-Growth Polymerization: Overview
2.5K
The polymerization process that involves carbanion as an intermediate is called anionic polymerization. It is also a type of addition or chain-growth polymerization. Anionic polymerization gets initiated by a strong nucleophile such as an organolithium or a Grignard reagent. The most commonly used initiator for anionic polymerization is butyl lithium. Monomers involved in anionic polymerization must possess a vinyl group bonded to one or two electron-withdrawing groups. For instance,...
2.5K
Molecular Weight of Step-Growth Polymers
2.7K
Step growth polymerization involves bi or multifunctional monomers. Bifunctional monomers react to form linear step growth polymers, whereas multifunctional monomers react to form non-linear or branched polymers.
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...
2.7K
Colloids
20.5K
Children at play often make suspensions such as mixtures of mud and water, flour and water, or a suspension of solid pigments in water known as tempera paint. These suspensions are heterogeneous mixtures composed of relatively large particles that are visible to the naked eye or can be seen with a magnifying glass. They are cloudy, and the suspended particles settle out after mixing. On the other hand, a solution is a homogeneous mixture in which no settling occurs and in which the dissolved...
20.5K