在2D材料中使用纳米缩的激子能量的局部应变工程

Kristyna Yang1, Yucheng Yang1, Daniel A Rhodes2

  • 1Department of Aerospace and Mechanical Engineering, University of Notre Dame, Notre Dame, IN 46556, USA. mrosenb2@nd.edu.

Nanoscale
|February 16, 2026
PubMed
概括

研究人员开发了一种新方法,可以精确控制WSe2.2等二维材料中的局部应变. 这种技术允许大,精确定义的应变场,对于理解和调整光电子特性至关重要.

相关概念视频

Strain Energy01:13

Strain Energy

Strain energy is a fundamental concept in the field of materials science and structural engineering, describing the energy absorbed by a material or structure when it is deformed under load.
Consider a rod that is fixed at one end and subjected to an axial force at the free end. This axial force induces stress within the rod, leading to its elongation. As the axial force increases, so does the elongation of the rod, illustrating a direct relationship between the force applied and the resulting...
1.0K
Elastic Strain Energy for Shearing Stresses01:20

Elastic Strain Energy for Shearing Stresses

As discussed in previous lessons, strain energy in a material is the energy stored when it is elastically deformed, a concept crucial in materials science and mechanical engineering. This energy results from the internal work done against the cohesive forces within the material. When a material undergoes shearing stress and corresponding shearing strain, the strain energy density, which is the energy stored per unit volume, is calculated. Within the elastic limit, where the stress is...
527
Elastic Strain Energy for Normal Stresses01:22

Elastic Strain Energy for Normal Stresses

Strain energy quantifies the energy stored within a material due to deformation under loading conditions, a fundamental concept in materials science and engineering. The strain energy can be modeled when a material is subjected to axial loading with uniformly distributed stress. In this scenario, the stress experienced by the material is the internal force divided by the cross-sectional area, and the strain induced is directly proportional to this stress through the modulus of elasticity.
If...
626