通过优化陶介层厚度来提高Cr3C2-NiCr/AlCrN双重涂层的高温 Tribological 性能

Feng Mao1, Dongqing He1, Xiangxiang Pan1

  • 1State Key Laboratory of Advanced Processing and Recycling of Non-ferrous Metals, Lanzhou University of Technology, Lanzhou 730050, China.

概括

优化Cr3C2-NiCr间层厚度是高温性能的关键. 在Cr3C2-NiCr/AlCrN双重涂层中的100微米中间层可以防止磨损并增强650°C的tribological特性.