概括
在碳纤维增强聚合物 (CFRP) 结合钢结构中检测早期解结损伤是具有挑战性的. 混合频超声波导向波有效地识别了接吻纽带,损伤严重程度与非线性参数相关.
科学领域:
- 材料科学 材料科学 材料科学
- 结构工程 结构工程
- 非破坏性测试 不破坏性测试
背景情况:
- 碳纤维增强聚合物 (CFRP) 层层增强钢结构.
- 解锁损害,特别是亲吻债券,对CFRP增强结构构成了关键威胁.
- 传统的超声波方法由于微尺度损伤和接口波的复杂性,难以在早期检测亲吻纽带.
研究的目的:
- 提出和验证一种用于识别和评估CFRP钢结构中接吻键损伤的新方法.
- 使用具有非线性特征的混合频超声波导向波用于损害评估.
- 为了比较不同波形模式的灵敏度,用于接吻键检测.
主要方法:
- 开发一个有限元模型来模拟接吻键和波相互作用.
- 拟议检测方法的实验验证.
- 基于损坏引起的和差频率计算非线性参数.
- 采用混合频率引导波激发,具有不同的波形模式.
主要成果:
- 非线性参数与接吻纽带的长度成比例增加.
- 模拟和实验结果都证实了拟议方法的有效性.
- 这项研究量化了非线性参数与亲吻纽带严重程度之间的关系.
结论:
- 混合频超声波导向波为在CFRP结合钢结构中识别和评估接吻键损伤提供了一种有效的方法.
- 非线性参数提供了一种可靠的定量衡量方法,用于评估亲吻关系的严重程度.
- 开发的方法增强了CFRP增强组件的结构完整性监测.
更多相关视频
07:37Full-field Strain Measurements for Microstructurally Small Fatigue Crack Propagation Using Digital Image Correlation Method
Published on: January 16, 2019
10.2K
05:30Crack Monitoring in Resonance Fatigue Testing of Welded Specimens Using Digital Image Correlation
Published on: September 29, 2019
8.8K
相关概念视频
Microcracking in Concrete
621
Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
621
Fiber Reinforced Concrete
647
Fiber-reinforced concrete significantly enhances the structural and nonstructural properties of traditional concrete by incorporating fibers like steel, glass, and polymers. These fibers, varying from natural ones such as sisal and cellulose to manufactured ones like polypropylene and Kevlar, are mixed into hydraulic cement with aggregates. Steel fibers, often preferred for their robustness, contribute to improved ductility, toughness, and post-cracking performance. The concrete is classified...
647
Corrosion of Reinforcement
752
The corrosion of steel reinforcement within concrete is a process influenced by the material's inherent properties and external factors. The high pH level of around 13, provided by calcium hydroxide present in concrete, initially protects the steel reinforcement by promoting the formation of a passive iron oxide layer on its surface.
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
752