P E Cardoso1, R R Braga, M R Carrilho
1Department of Dental Materials, School of Dentistry, University of Sao Paulo, Brazil.
Objectives:
The aim of this study was to determine bond strength between dentin and three adhesive systems, by means of microtensile, shear and tensile tests.
Methods:
Extracted human molars were embedded in acrylic resin and had the dentin exposed on three of their smooth surfaces. On each surface a specimen was prepared to be submitted to either micro-tensile, shear or tensile bond strength testing. For shear and tensile tests, after adhesive application, a cone 3 mm high and diameter of 3 mm in the small surface was built with composite resin. The shear test was performed with a chisel. Tensile testing was made by pulling the resin cone via a metallic clamp. For micro-tensile testing, composite approximately 5 mm high was placed over the entire exposed dentin. Then, using a diamond disk perpendicular to the bonding interface, 'sticks' with 0.25 mm2 rectangular cross-sectional area were obtained and subjected to tensile force.
Results:
All tests ranked the adhesives in the same order. Mean values obtained by the micro-tensile test were not statistically different. For shear and tensile tests, Single Bond gave higher bond strength than Etch & Prime 3.0 (p < 0.05). Scotchbond Multi-Purpose Plus originated bondings that were statistically similar to both Single Bond and Etch & Prime 3.0. Comparing the three tests, a higher mean (p < 0.05) and a smaller coefficient of variation were found with the micro-tensile test.
Significance:
The one-bottle adhesive system obtained higher bond strength values than the self-etching adhesive upon shear and tensile strength tests. Depending on the test applied, differences among materials may not be disclosed.
Related Concept Videos
Tension Response at Adherens Junctions
α-Catenin as a Mechanosensory Protein
The α-catenin of adherens junctions is an allosteric protein with three VH (vinculin homology) domains...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
Bonding and Strength of Aggregate
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen also...
Relation Between Tensile Strength and Compressive Strength of Concrete
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used to...