Related Experiment Videos

Surface analysis of a femoral stem after failed total hip replacement

G Maccauro1, C Piconi, L Pilloni

  • 1Dept. of Orthopaedics, Catholic University of Rome, Italy.

International Orthopaedics
|November 18, 2000
PubMed